COOLTHERM 6733

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM 6733

Main features

  • Solvent-Free RTV Silicone Encapsulation
  • Low-Stress No-Exotherm Room-Temperature Cure
  • -60 to 205 deg C Continuous Service

Product Description

CoolTherm® Circalok 6733 Silicone System is the hardener component used with Circalok® 6716 Silicone Resin to create a two-component, solvent-free RTV silicone encapsulant system for potting and encapsulating low- and high-voltage electrical and electronic assemblies. The cured system provides low stress, excellent dielectric properties, room-temperature curing without hardener poisoning, and cures without exotherm, making it suitable for protecting sensitive electronic components.

Key Features

  • Forms a two-component solvent-free RTV silicone encapsulant with Circalok® 6716 Resin.
  • Room-temperature curing formulation that is not subject to hardener poisoning.
  • Low-shrinkage, low-stress cure helps protect sensitive electronic assemblies.
  • Cures without exotherm, including deep-section encapsulations.
  • Provides excellent dielectric strength and electrical resistivity after cure.
  • Supports continuous operating temperatures from -60°C to +205°C.

Suitable For

  • Potting electrical assemblies
  • Encapsulating electronic assemblies
  • Low-voltage electronics
  • High-voltage electronic assemblies
Product Family

COOLTHERM 6733

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
Mix Ratio
100:2.5

Additional Information

As-Supplied / Before-Processing Properties

Property Value
Compatible Resin Circalok® 6716 Silicone Resin
Mix Ratio (Resin : Hardener) 100 : 2.5 by weight
Working Life 45 minutes @ 25°C
Cure Time 12–16 hours @ 25°C
Shelf Life 6 months at 25°C in the original unopened container

After-Processing / Final-State Properties

Property Value
Thermal Conductivity 0.3 W/m·K (ISO 22007-2)
Coefficient of Thermal Expansion 110 ppm/°C
Hardness Shore A 45
Tensile Strength 0.97 MPa (140 psi)
Elongation at Break 200%
Volume Resistivity 1 × 1015 ohm·cm
Dielectric Strength 19.7 kV/mm (500 V/mil) (ASTM D149)
Dielectric Constant 3.5 @ 25°C (ASTM D150)
Dissipation Factor 0.01 @ 25°C (ASTM D150)

Leading Brands Trust in Our Products and Services