COOLTHERM 6053

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM 6053

Main features

  • Flexible Cured Material
  • Heat & Oxidation Resistance
  • Supplied in a 16-Ounce Aerosol Format

Product Description

Circalok™ 6053 Mold Release Agent is an aerosol-applied mold release formulation based on organic and silicone polymers. Formerly identified as EMR-1023, it is intended to release epoxy, polyester, synthetic rubber, and flexible or rigid urethane molding compounds, including TDI- and MDI-based urethane elastomers and polyether or polyester urethane foams. The formulation is described as heat resistant, oxidation resistant, and capable of forming a high-strength release film that helps protect mold surfaces and limit mold buildup. Circalok 6053 is supplied in 16-ounce aerosol cans for direct application to molding tools.

Key features

  • Broad molding-compound coverage: Supports release of epoxy, polyester, synthetic rubber, urethane elastomers, and flexible or rigid urethane foams.
  • Heat- and oxidation-resistant release film: Combines documented heat resistance, oxidation resistance, and high film strength.
  • Aerosol application format: Supplied in 16-ounce aerosol cans for application to mold surfaces.

Applications / Suitable for

  • Reaction injection molding
  • Direct injection molding
  • Casting and transfer molding
  • Potting and laminating processes
Product Family

COOLTHERM 6053

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Organic and silicone polymers
Product Type
Aerosol

Additional Information

Technical properties

As-supplied / before-processing properties

Supported product identity, formulation, and supply-format information before application to the mold surface.

Property Value Unit Method / condition
Product type Mold release agent — Aerosol-applied formulation
Formulation Organic and silicone polymers — General formulation description
Package format 16 ounce aerosol can Available supply format stated in DS3713