CONATHANE PR-1167

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

CONATHANE PR-1167

Main features

  • Single-Component Polyurethane Primer for Cured Polyurethane
  • May Be Applied by Spray
  • 75 cP Application Viscosity

Product Description

CONAP® PR-1167 Polyurethane Primer is a single-component, solvent-borne isocyanate prepolymer primer for bonding liquid polyurethane molding and potting compounds to difficult substrates. Documented substrates include cured polyurethane, neoprene rubber, and cadmium-plated metals. The light-amber primer may be applied by spray, dip, or brush and is allowed to air dry for one to two hours or until tack-free before the polyurethane is introduced. Typical as-supplied properties include 75 cP viscosity, 58% solids content, and 1.02 specific gravity at 25°C.

Key features

  • Polyurethane bonding primer: The primer is used with liquid polyurethane molding and potting compounds.
  • Multiple application methods: It may be applied by spray, dip, or brush.
  • Controlled as-supplied properties: Typical viscosity is 75 cP with 58% solids content.

Applications / Suitable for

  • Bonding polyurethane compounds to cured polyurethane
  • Priming neoprene rubber
  • Priming cadmium-plated metals
Product Family

CONATHANE PR-1167

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
light amber
Specific Gravity
1.02
Physical Properties
Viscosity
75 mPa.s
Thermal Properties
Flash Point
27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Single-component primer N/A As supplied
Color Light amber N/A As supplied
Viscosity 75 cP At 25°C
Solids content 58 % 135°C for 45 min
Specific gravity 1.02 N/A At 25°C
Flash point 27 °C ASTM D93
Air-dry time 1 to 2 h Or until tack-free
Shelf life 12 months At or below 25°C in original sealed containers

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers