CONATHANE AD-6415

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONATHANE AD-6415

Main features

  • Two-Part Polyurethane Adhesive
  • 1:2 Cartridge or Bulk
  • Filtration Membrane Bonding

Product Description

CONAP AD-6415 Polyurethane Adhesive is a two-component, unfilled polyurethane adhesive and sealant for filtration membrane assemblies. The product is supplied in 1:2 cartridge and bulk formats for controlled component proportioning during application. It is designed for bonding and sealing ceramic and flat-sheet filtration membranes, combining adhesive and sealing functions within the supported assembly process. Component preparation, mixing, dispensing and cure conditions should follow the requirements for the selected package. The complete two-part configuration must be used to develop the intended bonded and sealed assembly.

Key features

  • Two-Component Polyurethane: combines an unfilled resin and curative system for bonding and sealing
  • 1:2 Processing Format: is supplied in cartridge or bulk configurations for controlled proportioning
  • Filtration Membrane Application: supports ceramic and flat-sheet membrane bonding and sealing

Applications

Bonding and sealing ceramic and flat-sheet filtration membranes.

Product Family

CONATHANE AD-6415

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Mechanical Properties
Elongation
520 %
Physical Properties
Viscosity
15,000 mPa.s