CONAPOXY RN-1000

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONAPOXY RN-1000

Main features

  • Amber Epoxy Potting and Casting Resin Compatible
  • 24-Hour 25 deg C Cure
  • Three Curing-Agent Systems

Product Description

CONAPOXY® RN-1000 Epoxy Encapsulant Resin is an amber epoxy resin for potting and casting when combined with CONACURE EA-02, EA-028, or EA-87 curing agent. The three documented systems cure at room temperature or with heat and are positioned for epoxy encapsulation where electrical properties, thermal-shock resistance, low exotherm, and low shrinkage are required. The resin has a listed specific gravity of 1.13. Mix ratio, mixed viscosity, Shore D hardness, tensile strength, and volume resistivity vary with the selected curing agent, so the system configuration must remain explicit.

Key features

  • Potting and casting resin: The amber epoxy resin is used with CONACURE EA-02, EA-028, or EA-87.
  • Room-temperature or heat cure: Each documented system cures for 24 hours at 25°C or two hours at 60°C.
  • Hardener-dependent properties: Mix ratio, mixed viscosity, hardness, tensile strength, and volume resistivity vary by curing agent.

Applications / Suitable for

  • Epoxy potting and casting
  • Electrical and electronic encapsulation
  • Systems using CONACURE EA-02, EA-028, or EA-87
Product Family

CONAPOXY RN-1000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
800 mPa.s
General Properties
Color
amber
Specific Gravity
1.14

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin color Amber N/A As supplied
Resin specific gravity 1.13 N/A As supplied
Mix ratio with EA-02 100:11 parts by weight Resin : curing agent
Mixed viscosity with EA-02 600 cP At 25°C
Mix ratio with EA-028 100:28 parts by weight Resin : curing agent
Mixed viscosity with EA-028 500 cP At 25°C
Mix ratio with EA-87 100:37 parts by weight Resin : curing agent
Mixed viscosity with EA-87 250 cP At 25°C
Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin color Amber N/A As supplied
Resin specific gravity 1.13 N/A As supplied
Mix ratio with EA-02 100:11 parts by weight Resin : curing agent
Mixed viscosity with EA-02 600 cP At 25°C
Mix ratio with EA-028 100:28 parts by weight Resin : curing agent
Mixed viscosity with EA-028 500 cP At 25°C
Mix ratio with EA-87 100:37 parts by weight Resin : curing agent
Mixed viscosity with EA-87 250 cP At 25°C