CONAPOXY FR-1274

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONAPOXY FR-1274

Main features

  • 1:1 Meter-Mix Processing
  • Long Low-Exotherm Work Window
  • UL 94 V-0 at 3 mm

Product Description

CONAPOXY FR-1274 Epoxy Encapsulant is a two-component, mineral-filled, flame-retardant epoxy system for potting and casting electrical and electronic devices. Its 1:1 mix ratio by both weight and volume accommodates hand mixing, meter mixing and vacuum potting. The mixed material has an initial viscosity of 40,000 cP at 25 deg C, a 2 to 3 hour gel time for a 225 g mass, and low-exotherm behavior. The system is used to pot and encapsulate modules, transformers, coils, circuitry and strain-sensitive devices.

Key features

  • 1:1 Weight and Volume Mix: uses equal component ratios for hand, meter-mix and vacuum potting methods
  • Long Low-Exotherm Window: combines a 2 to 3 hour gel time for a 225 g mass with a 43 deg C peak exotherm for a 200 g mass
  • UL 94 V-0 at 3 mm: provides a V-0 flame classification for the cured system at 3 mm thickness

Applications

Potting and encapsulation of modules, transformers, coils, circuitry and strain-sensitive electrical or electronic devices.

Product Family

CONAPOXY FR-1274

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.6
Thermal Properties
Glass Transition Temperature (Tg)
50 °C
Thermal Conductivity
0.8 W/m.K
UL 94 Rating
v0
Electrical Properties
Dielectric Strength
15.75 kV/mm
Surface Resistivity
3.0 x 10^17 Ohms/sq
Volume Resistivity
8.0 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for FR-1274 Part A, Part B and mixed material; the applicable state is identified by row.

PropertyValueUnitMethod / condition
Part A viscosity27,000cP25 deg C
Part B viscosity55,000cP25 deg C
Specific gravity1.6Part A and Part B at 25 deg C
Mix ratio100:100partsBy weight and by volume
Initial mixed viscosity40,000cP25 deg C
Gel time2 to 3hours225 g mixed mass at 25 deg C
Peak exotherm43deg C200 g mixed mass at 25 deg C
Shelf life12monthsOriginal sealed containers; dry storage below 25 deg C, out of direct sunlight
Technical properties

After-processing / final-state properties

Values are typical for cured FR-1274 and are not specification limits.

PropertyValueUnitMethod / condition
Dielectric strength400V/milASTM D149 at 25 deg C
Volume resistivity8.0 x 10^14ohm-cmASTM D257 at 25 deg C
Shore hardnessD 80ASTM D2240 at 25 deg C
Tensile strength5,500psiASTM D412 at 25 deg C
Linear shrinkage0.1%ASTM D2566 at 25 deg C
Glass transition temperature50deg CCured material
Thermal conductivity0.8W/(m K)ASTM D5930
FlammabilityV-0UL 94 at 3 mm