CNP OM350

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

CNP OM350

Main features

  • Fine-feature no-clean solder paste with demonstrated Pin-in-Paste performance and robust solderability across OSP-Cu, Immersion Ag, Immersion Sn, ENIG, and lead-free HASL finishes.
  • Greater than 6-hour stencil life at 25 °C with stable storage and handling performance up to 30 °C for 21 days.
  • Halide-free ROL0 formulation with IPC Class III voiding performance and documented SIR and electromigration reliability results.

Product Description

ALPHA OM-350 Solder Paste is a lead-free, no-clean solder paste designed for fine-feature printing and demanding SMT reflow processes in air or nitrogen. Its broad reflow process window supports soldering on OSP-Cu, Immersion Ag, Immersion Sn, ENIG, and lead-free HASL surface finishes, including applications involving CSP and QFN components. ALPHA OM-350 combines stable paste viscosity with long stencil life and high tack force to support consistent printing and pick-and-place performance. The halide-free formulation is classified ROL0 according to IPC J-STD-004 and meets IPC Class III voiding performance.

Key features

  • Fine-feature and Pin-in-Paste capability: Supports fine-feature printing and demonstrated Pin-in-Paste performance for printing, dispensing, or pin-transfer SMT applications.
  • Long stencil life and stable viscosity: Provides greater than 6 hours of stencil life at 25 °C and stable handling up to 30 °C for 21 days.
  • Wide reflow process window: Supports straight-ramp and soak profiles in both air and nitrogen across multiple lead-free board finishes.
  • Controlled voiding and solder balling: Meets IPC Class III voiding performance and is formulated to reduce random solder ball levels.

Applications / Suitable for

  • Fine-feature SMT stencil printing
  • Pin-in-Paste / Paste-in-Hole assembly
  • High-density PWB assemblies
  • Assemblies using CSP and QFN components
Product Family

CNP OM350

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
SAC305; SACX Plus 0307; Innolot; Sn5/Pb92.5/Ag2.5

Additional Information

Technical properties

As-supplied / before-processing properties

Selected properties and available configurations of ALPHA OM-350 before reflow.

Property Value Method or condition
Available alloys SAC305, SACX Plus 0307, Innolot, 5Sn92.5Pb2.5Ag Other Sn-Ag-Cu alloys available upon request
Powder size Type 3, Type 4, Type 5 Available configurations
Flux residue Approximately 5% By weight
Flux classification ROL0 IPC J-STD-004
Halide content Halide free By titration and IC, IPC J-STD-004
Metal content - Type 4 89.0% M16 designation; Malcom Spiral Viscometer, JIS Z 3284 Annex 6
Metal content - Type 5 88.8% M16 designation; Malcom Spiral Viscometer, JIS Z 3284 Annex 6
Stencil life >6 hours 25 °C (77 °F)
Technical properties

After-processing / final-state properties

Selected electrical reliability and soldering performance results for ALPHA OM-350 under the stated test conditions.

Property Result Method or condition
IPC SIR Pass, 1.8 x 1010 ohms IPC J-STD-004; 168 hours at 85 °C/85% RH; pass >=1 x 108 ohm
Bellcore SIR Pass, 1.9 x 1012 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass >=1 x 1011 ohm
Electromigration Pass; initial 7.8 x 108 ohms, final 8.2 x 109 ohms Bellcore GR78-CORE; 10 V, 500 hours; pass = final > initial/10
HP ECM test Pass; no migration after 28 days 50 °C/90% RH, 5 V; Cu/ImmAg/ImmSn finishes; Hewlett-Packard EL-EN861-00
Copper corrosion Pass IPC J-STD-004 and JIS Z 3197:1986
Voiding performance Class III IPC voiding classification

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers