CNP OM338T

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

CNP OM338T

Main features

  • Ultra-fine feature solder paste supporting full alloy coalescence on circular dimensions as small as 0.25 mm with a 0.100 mm stencil.
  • High-throughput printing at speeds up to 200 mm/s with greater than 8-hour stencil life at 50% RH and 23 °C.
  • ROL0, halide-free no-clean formulation with IPC-7095 Class III voiding performance and documented electrical reliability.

Product Description

ALPHA OM-338-T Ultra Fine Feature Lead-Free Solder Paste is a lead-free, no-clean solder paste designed for standard and fine-pitch stencil printing across a broad range of electronics assembly applications. Also identified as ALPHA OM-338 with M13 viscosity, it combines ultra-fine feature repeatability with a broad processing window and print speeds up to 200 mm/s. The paste provides good solderability on CuOSP and other board and component finishes, with resistance to random and mid-chip solder balling. ALPHA OM-338-T is ROL0 classified, halide-free, compatible with air or nitrogen reflow, and meets IPC-7095 Class III voiding performance.

Key features

  • Ultra-fine feature capability: Supports full alloy coalescence on circular dimensions as small as 0.25 mm (0.010 in) using a 0.100 mm (4 mil) stencil.
  • High-throughput printing: Supports print speeds from 25 to 200 mm/s (1 to 8 in/s) with stencil life greater than 8 hours at 50% RH and 23 °C.
  • Wide reflow process window: Provides good solderability across various board and component finishes and is compatible with clean-dry air or nitrogen reflow.
  • Controlled voiding and solder balling: Meets IPC-7095 Class III voiding performance and is designed to reduce random solder balling.

Applications / Suitable for

  • Standard and fine-pitch stencil printing
  • Ultra-fine feature electronics assembly
  • High-throughput SMT processing
  • Lead-free assembly using air or nitrogen reflow
Product Family

CNP OM338T

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
SAC305; SAC387; SAC396; SAC405; SACX alloys

Additional Information

Technical properties

As-supplied / before-processing properties

Selected properties and available configurations of ALPHA OM-338-T before reflow.

Property Value Method or condition
Available alloys SAC305, SAC387, SAC396, SAC405, SACX Plus 0307, SACX Plus 0807 e1 alloys per JESD97 Classification
Powder size Type 3 (25-45 µm); Type 4 by special request Type 3 per IPC J-STD-005; technical data developed using Type 3 powder
Metal load 88.5% OM-338-T M13 viscosity designation for printing
Flux classification ROL0 IPC J-STD-004A
Halide content Halide free By titration; passes Ag Chromate Test, IPC J-STD-004A
Stencil life >8 hours 50% RH, 23 °C (74 °F)
Technical properties

After-processing / final-state properties

Selected electrical reliability and soldering performance results for ALPHA OM-338-T under the stated test conditions.

Property Result Method or condition
SIR Pass, >1.9 x 1010 ohms IPC J-STD-004A; 7 days at 85 °C/85% RH; pass >=1 x 108 ohm
SIR Pass, 8.3 x 1012 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass >=1 x 1011 ohm
Electromigration Pass; initial 5.3 x 1010 ohms, final 1.5 x 1011 ohms Bellcore GR78-CORE; 65 °C/85% RH, 10 V, 500 hours; pass = final > initial/10
Voiding performance Class III IPC-7095 voiding performance classification
Copper corrosion Pass, no evidence of corrosion IPC J-STD-004A