CHEMLOK 6411

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

CHEMLOK 6411

Main features

  • 30-Minute Room-Temperature Dry
  • 12.7 to 25.4 um Film
  • Brush, Roll, Dip or Spray

Product Description

Chemlok 6411 Adhesive is a one-part, solvent-based, heat-reactive covercoat adhesive for bonding supported rubber compounds to metal and other rigid substrates. For general use, it is applied over Chemlok 205 or 207 primer, although selected systems may use it as a one-coat adhesive. Chemlok 6411 can be applied by brush, roll coat, dip, or spray and is used at a dry film thickness of 12.7 to 25.4 um. The applied film typically dries in about 30 minutes at room temperature, with hot-air drying available at temperatures up to 90 deg C.

Key features

  • Primer-System Flexibility: normally used over Chemlok 205 or 207 primer, with selected one-coat applications also supported
  • Multi-Method Application: applies by brush, roll coat, dip, or spray
  • Room-Temperature Drying: applied film typically dries in approximately 30 minutes at room temperature

Applications

Bonding supported rubber compounds to metal and other rigid substrates, normally with the specified Chemlok primer system.

Product Family

CHEMLOK 6411

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black Liquid
Density
970 -1010 kg/m3
Solids
22 - 26 %
Solvent
Xylene
Physical Properties
Viscosity
200 - 600 mPa.s
Thermal Properties
Flash Point
25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceBlack liquidTypical
Viscosity200 to 600cps25 deg C; Brookfield LVT, spindle 2, 30 rpm; typical
Density970 to 1010kg/m^3Typical
Solids by weight22 to 26%Typical
Flash point25deg CSeta; typical
Shelf life1yearBelow 25 deg C; original unopened container