CG 1305

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CG 1305

Main features

  • Medium Density Syntactic
  • High-Strength Structural Bonding
  • Pourable Bonding Material

Product Description

Huntsman CG-1305 Resin/Hardener Epoxy Syntactic is a medium-density, pourable epoxy syntactic system developed for aircraft production and industrial applications that require a combination of high strength and low weight. The two-component system is designed for reinforcing high-stress areas in honeycomb structures and for potting applications. CG-1305 offers good handling characteristics, a density of 0.90 g/cc maximum when mixed, and extended working time with a gel time exceeding 60 minutes at 25°C. The material is qualified to BMS 5-28 Type 7 Class 1 and develops compressive strengths up to 9.0 ksi after elevated-temperature cure schedules, making it suitable for structural reinforcement and lightweight filling applications.

Key features

  • Medium-density syntactic epoxy: Combines low weight and structural strength for aerospace and industrial reinforcement applications.
  • Pourable processing characteristics: Mixed viscosity of approximately 21,500 cP and gel time greater than 60 minutes at 25°C support handling and placement.
  • BMS-qualified performance: Qualified to BMS 5-28 Type 7 Class 1 and capable of achieving compressive strengths up to 9.0 ksi after cure.

Applications / Suitable for

  • Reinforcing high-stress areas in honeycomb structures
  • Aircraft production assemblies
  • Potting applications
  • Lightweight structural filling applications
Product Family

CG 1305

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Off-white
Component System
Two (Resin / Hardener)
Density (g)
0.90 max. g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Representative handling and processing properties of the mixed CG-1305 epoxy syntactic system.

Property Value Unit Method / condition
Color Off-white - Mixed material
Density 0.90 max. g/cc ASTM D792, mixed
Viscosity 21,500 cP 25°C, ASTM D2196
Gel Time >60 min 60 g mass at 25°C, ASTM D2471
Mix Ratio 100:20 wt. Resin : Hardener
Shelf Life 12 months Unopened containers at 25°C
Technical properties

After-processing / final-state properties

Typical cured-property data. Values are not intended as specifications.

Property Value Unit Method / condition
Compressive Strength 8.8 ksi ASTM D695, RT gel + 90 min @ 127°C
Compressive Modulus 420 ksi ASTM D695, RT gel + 90 min @ 127°C
Lap Shear Strength 1800 psi Al/Al, ASTM D1002, RT gel + 90 min @ 127°C
Weight Gain 0.50 % 24 h distilled water immersion, ASTM D543
Flammability Burn Rate 3 max. in./min 12-second vertical burn