BOSTIK 940FS

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 940FS

Main features

  • 10-Minute Cure Cycle
  • Adhesion and Mechanical Performance of Polyurethane
  • Primerless Glass-to-Aluminum Bonding

Product Description

Bostik Marine 940 Fast Set Adhesive/Sealant is a one-component, rapidly moisture-curing adhesive and sealant based on Silyl Modified Polymer (SMP) technology. Designed for demanding marine environments, it combines the adhesion and mechanical performance of a polyurethane with the flexibility and UV resistance of a silicone. The solvent-free, isocyanate-free formulation provides permanent elastic bonding, excellent weatherability, fast skin formation, and strong primerless adhesion to many marine substrates for above- and below-the-waterline applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Fast-setting SMP adhesive with approximately 10-minute skin time and one-day cure for rapid assembly.
  • Primerless adhesion to aluminum, steel, fiberglass, EPDM rubber, PVC, glass, and painted surfaces in many applications.
  • Excellent UV and weather resistance with permanent elasticity from -40°C to 100°C.
  • Solvent-free and isocyanate-free formulation that is paintable after skin formation and sandable after full cure.

Applications / Suitable For

  • Marine bonding and sealing
  • Above- and below-the-waterline applications
  • Deck hardware installation
  • Through-hull fittings
  • Rub rails
  • Porthole sealing
  • Bonding aluminum, steel, fiberglass, EPDM rubber and PVC components
Product Family

BOSTIK 940FS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
SMP marine adhesive/sealant
Thermal Properties
Operating Temperature
-40°C to +100°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Silyl Modified Polymer (SMP) — One-component moisture curing
Work life / Open time 15 minutes Typical uncured property
Skin time 10 minutes Typical uncured property
Curing time 1 day 77°F / 50% RH / 0.125 in. bead
Application temperature 40–95 (5–35) °F (°C) Recommended application range
Green strength 2.3 lb-force/ft² 0.125 in. thick, without sag
Shelf life 18 months (cartridges); 12 months (sausages) — Stored between 40°F and 80°F (5°C to 27°C)
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness 55 Shore A After 14 days at 77°F and 50% RH
Specific gravity 1.4 g/mL Typical cured property
Tensile strength @ 100% 400 psi Typical cured property
Tensile strength @ break 450 psi Typical cured property
Tensile shear strength 375 psi Aluminum-to-aluminum, 0.08 in. bondline
Elongation 225 % Typical cured property
Temperature resistance -40 to 212 (-40 to 100) °F (°C) Maintains elasticity in service
UV / Weather resistance Excellent — Supplier classification
Paintability After skin formation — Supplier recommendation
Sandability After full cure — Supplier recommendation