BOSTIK 920

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 920

Main features

  • Flexible Cured Adhesive
  • Above- and Below-the-Waterline Sealing and Bonding
  • Plastic, Wood, and FRP Bonding

Product Description

Bostik Marine 920 Urethane Adhesive/Sealant is a one-component, moisture-curing, gun-grade polyurethane adhesive and sealant formulated for above- and below-the-waterline marine sealing and bonding applications. The cured elastomeric seal provides excellent tear and abrasion resistance while maintaining permanent flexibility and strong adhesion to common marine substrates including wood, metals, fiberglass-reinforced plastic (FRP), and most plastics. It can be used as either an adhesive or a sealant for a wide range of marine assembly and maintenance applications.

Key Features

  • One-component moisture-curing polyurethane forms a tough, resilient elastomeric seal.
  • Excellent adhesion to wood, metals, fiberglass-reinforced plastic (FRP), and most plastics.
  • Excellent tear and abrasion resistance while maintaining permanent flexibility.
  • Suitable above and below the waterline for marine sealing and bonding applications.

Applications / Suitable For

  • Above- and below-waterline marine sealing
  • Deck-to-hull assembly
  • Hull seams
  • Keel joints
  • Sealing around marine windows and doors
  • Under moldings
Product Family

BOSTIK 920

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Polyurethane adhesive/sealant
Thermal Properties
Operating Temperature
-40°F to +180°F (intermittent) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology One-component polyurethane adhesive/sealant — Moisture curing
Tool / work life 70 minutes Typical uncured property
Tack-free time 6 hours Typical uncured property
Curing time 3–6 days 77°F (25°C)
Flow, sag or slump 0.1 inch Typical uncured property
Staining None — Typical uncured property
Shelf life 12 months — Stored at or below 80°F (27°C)
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness 38 Shore A After 14 days at 77°F and 50% RH
Modulus @ 100% elongation 70 psi Typical cured property
Tensile strength 180 psi Typical cured property
Elongation 950 % Typical cured property
Adhesion in peel >35 piw Typical cured property
Joint movement capability ±25 % Typical cured property
Ozone resistance Excellent — Typical cured property
UV resistance Good — Typical cured property
Temperature resistance -40 to 180 °F Intermittent contact

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers