BOSTIK 1100 FS

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 1100 FS

Main features

  • 90-Minute Tack-Free Time
  • Plastic-to-Wood Urethane Bonding
  • +/-25% Joint Movement Capability and Temperature Resistance

Product Description

Bostik 1100 FS is a one-component, moisture-curing polyurethane adhesive and sealant for bonding, beading, and sealing applications. It cures to form a tough, flexible seal with adhesion to wood, metals, fiber-reinforced plastic, and most plastics. The non-sag formulation combines a 70-minute working life with a 90-minute tack-free time and is designed for general industrial, HVAC, and transportation assembly. The cured material provides ±25% joint movement capability, good UV resistance, and service-temperature resistance from -40 to 82°C (-40 to 180°F).

Key features

  • Fast-setting polyurethane: Moisture-cures to a tough, flexible seal with a 90-minute tack-free time.
  • Broad substrate adhesion: Provides adhesion to wood, metals, fiber-reinforced plastic, and most plastics.
  • Movement and environmental performance: Provides ±25% joint movement capability with excellent ozone resistance and good UV, heat, and aging resistance.

Applications / Suitable for

  • General industrial bonding, beading, and sealing
  • HVAC assembly
  • Truck, horse trailer, RV, emergency vehicle, bus, railcar, and container construction
Product Family

BOSTIK 1100 FS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
One-component polyurethane adhesive/sealant
Thermal Properties
Operating Temperature
-40°C to +90°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured properties and supplier storage information for Bostik 1100 FS.

Property Value Unit Method or condition
Tool / work life 70 minutes Typical uncured property
Tack-free time 90 minutes Typical uncured property
Curing time 1.5–3 days At 77°F
Flow, sag, or slump Nil — Typical uncured property
Shelf life 9 months From date of manufacture when stored at or below 80°F (27°C)
Technical properties

After-processing / final-state properties

Typical cured properties after 14 days at 77°F and 50% relative humidity.

Property Value Unit Method or condition
Hardness 40–45 Shore A After 14 days at 77°F and 50% RH
Elongation 850 % After 14 days at 77°F and 50% RH
Adhesion in peel Greater than 25 piw After 14 days at 77°F and 50% RH
Joint movement capability ±25 % Typical cured property
Temperature resistance -40 to 82 (-40 to 180) °C (°F) Typical cured property