BONDERITE S-FN GP 1904

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BONDERITE S-FN GP 1904

Main features

  • PTFE/Graphite Dry-Film Lubricant
  • Corrosion and Solvent Resistance
  • Multi-Substrate Dry Lubrication

Product Description

BONDERITE® S-FN GP 1904 ACHESON is a one-package resin-bonded dry film lubricant formulated with PTFE and graphite in a thermosetting binder. It is designed for spray, brush, or dip application to produce a durable, low-friction coating with excellent corrosion and solvent resistance. Its broad curing temperature range allows use on engineering metals as well as wood, rubber, and many plastics. :contentReference[oaicite:0]{index=0}

Key Features

  • PTFE and graphite dry film lubricant providing low-friction performance.
  • Excellent corrosion and solvent resistance after curing.
  • One-package formulation suitable for spray, brush, or dip application.
  • Wide curing temperature range for compatibility with metals, wood, rubber, and many plastics.
  • Flexible coating with consistent spray and dip-spin application characteristics.

Applications / Suitable for

  • Fasteners
  • Sliding rails
  • Lock mechanisms
  • Seat belt components
  • Latches
  • Mechanical assemblies
Product Family

BONDERITE S-FN GP 1904

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type
PTFE/graphite dry-film lubricant

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Dry film lubricant — Supplier classification
Pigment PTFE and graphite — Wet product
Binder Thermoset — Wet product
Appearance Black liquid — Wet product / SDS
Carrier MEK or BONDERITE L-FG SB-2 ACHESON — Supplier description
Viscosity 100 mPa·s (cP minimum) Typical
Density / Specific Gravity 0.96 (0.959 SDS) kg/L Typical
Solids content 25 % by weight Typical
Flash point 8°C (TDS); 7.78°C closed cup (SDS) °C Typical
VOC 720 g/L Typical
Recommended storage temperature 5–30 °C SDS
Shelf life Not stated — Refer to product label or TDS
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Coating color Black — Cured coating
Coefficient of friction 0.08–0.10 — Static
Recommended dry film thickness 0.008–0.025 mm 0.0003–0.0010 in
Theoretical coverage 6.81 m²/kg @ 25 µm dry film thickness
Continuous service temperature 149 °C 300°F
Salt spray resistance >96 hours ASTM B117 over zinc phosphated surface, 25 µm coating
Typical curing schedules 149°C / 60 min; 177°C / 10 min; 204°C / 8 min — Substrate temperature