BONDERITE S-FN 309

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BONDERITE S-FN 309

Main features

  • Fast-Drying PTFE Dry-Film Lubrication
  • Wood/Metal/Rubber/Plastic/Glass Surface Adhesion
  • Spray/Brush/Dip/Roller Application Methods

Product Description

BONDERITE® S-FN 309 ACHESON is a concentrated PTFE fluorocarbon resin dispersion in an isopropyl alcohol carrier designed to produce fast-drying, low-friction dry film lubrication when diluted or compounded into lubricant formulations. It provides good adhesion to a wide range of substrates, including wood, metal, rubber, plastic, and glass, helping moving parts operate more smoothly while reducing wear and maintenance requirements. :contentReference[oaicite:0]{index=0}

Key Features

  • Concentrated PTFE fluorocarbon resin dispersion for dry film lubrication.
  • Fast-drying, low-friction coating that improves lubrication performance.
  • Adheres to wood, metal, rubber, plastic, and glass.
  • Suitable for dilution or compounding into lubricant formulations.
  • Can be applied by spray, brush, dip, or roller.

Applications / Suitable for

  • Lubricant aerosol component
  • Sealed systems
  • Piano action parts
  • Tools
  • Solenoid plungers
  • Storage bins
  • Window guides
  • Moving parts on wood, metal, fabric, plastic, and rubber
Product Family

BONDERITE S-FN 309

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type
PTFE dry-film lubricant
Thermal Properties
Operating Temperature
Air dried; no service temperature specified °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Lubricant — Supplier classification
Product Type PTFE fluorocarbon resin dispersion — Concentrated dispersion
Carrier Anhydrous isopropyl alcohol — Supplier description
Lubricating solid PTFE — Supplier description
Viscosity 25–50 mPa·s @ 25°C
Solids content 20 % PTFE
Particle size 90% between 2–4 µm By volume
Density 0.923 kg/L @ 25°C
Flash point 11.7 °C 53°F
Color Translucent white — As supplied
VOC 683 g/L Reduced VOC: 764 g/L
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Recommended dilution 1:3 (product:diluent) — Initial evaluation
Application methods Spray, brush, dip, roller — Spray recommended for uniform coverage
Typical dry film thickness 0.2–0.5 mil Typical application
Coverage 8.1 m²/L @ 12.7 µm (0.5 mil)
Performance Fast-drying, low-friction coating — Finished dry film
Substrate compatibility Wood, metal, rubber, plastic, glass — Finished coating

Leading Brands Trust in Our Products and Services