BONDERITE C-AK MIL-ETCH

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BONDERITE C-AK MIL-ETCH

Main features

  • Uniform Fine Satin or Frosted Etch
  • Low-Foam Low-Mist Alkaline Etching
  • BAC 5786 Operating Conditions

Product Description

BONDERITE® C-AK MIL-ETCH AERO is a granular alkaline cleaner and etchant formulated to produce a fine satin or frosted etch on aluminum and its alloys. The working solution develops a low-foam blanket to minimize caustic mist while providing excellent sequestering action that helps prevent scale and sludge buildup on tanks and heating coils. It is designed for aluminum surface preparation prior to deoxidizing, anodizing, and other finishing operations. :contentReference[oaicite:0]{index=0}

Key Features

  • Produces a fine satin or frosted etch on aluminum and aluminum alloys.
  • Low-foam alkaline formulation helps reduce caustic mist generation during processing.
  • Excellent sequestering action minimizes scale and sludge buildup on tanks and heating coils.
  • Suitable for aluminum pretreatment prior to deoxidizing and anodizing.
  • Supports standard and BAC 5786 operating conditions.

Applications / Suitable for

  • Aluminum surface etching
  • Aluminum alloys
  • Pretreatment before deoxidizing
  • Pretreatment before anodizing
  • Aerospace metal finishing
Product Family

BONDERITE C-AK MIL-ETCH

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type
Granular alkaline cleaner and aluminum etchant
Thermal Properties
Operating Temperature
37-72; 32 - 43 (for BAC 5786) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Alkaline cleaner / etchant — Supplier classification
Physical form Granular powder — Supplier description
Application Aluminum etching and cleaning — Supplier description
Bath make-up 25–50 lb per 100 gal Initial bath preparation
Recommended storage Cool, dry, ventilated area in sealed containers — Away from acidic materials
Shelf life Not stated — Technical Process Bulletin
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Surface finish Fine satin or frosted etch — On aluminum and its alloys
General operating concentration 4–8 (30–60) oz/gal (g/L) General operation
General operating temperature 37–72 °C 100–160°F
General treatment time 5–10 minutes Optimum
BAC 5786 concentration 3–5 (22.5–37.5) oz/gal (g/L) Approved as additive only
BAC 5786 temperature 32–43 °C 90–110°F
BAC 5786 treatment time 5–10 minutes Optimum