Product Description

BONDERITE® C-AK 5948 R EU AERO is a blue, water-based alkaline cleaner concentrate formulated for cleaning painted and unpainted aircraft exterior and interior surfaces after dilution with water. Suitable for aircraft metals and well-bonded paint, it provides nonstaining, nonstreaking cleaning on aluminum and rinses freely after use. The product is designed for immersion and dip applications, including ultrasonic parts-cleaning systems, and is suitable for all models of jet aircraft.

Key features

  • Aircraft-surface compatibility: Suitable for aircraft metals, well-bonded paint, and painted or unpainted aircraft surfaces.
  • Aluminum appearance protection: Formulated to clean aluminum without staining or streaking under suitable process conditions.
  • Free-rinsing formulation: Readily soluble and stable in water mixtures for efficient rinsing after cleaning.
  • Immersion and ultrasonic use: Designed for dip tanks, immersion cleaning, and ultrasonic parts-cleaning systems.
  • Nonflammable concentrate: Supplied as a nonflammable liquid alkaline cleaner.

Applications / Suitable for

  • Painted and unpainted aircraft exterior surfaces
  • Aircraft interior surfaces
  • Aircraft metals and well-bonded paint
  • Immersion and dip cleaning
  • Ultrasonic parts-cleaning tanks
  • Metal pretreatment processes
Product Family

BONDERITE C-AK 5948-R

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
0–40°C °C
General Properties
Appearance
Blue liquid
Specific Gravity
1.01–1.02 g/cm³

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published characteristics and storage information for BONDERITE® C-AK 5948 R EU AERO.

Property Value Unit Method / condition
Technology Metal pretreatment — Supplier classification
Product type Alkaline cleaner — Supplier classification
Application Immersion — Supplier classification
Appearance Blue liquid — As supplied
pH 11.7–12.3 — 100% product at 20°C; potentiometric method
Density 1.01–1.02 g/mL At 20°C
Kinematic viscosity 1–10 mm²/s At 20°C
Water solubility Miscible — Qualitative, at 20°C
Flash point >100 °C Product classified as nonflammable
Storage temperature 0–40 °C Store cool and frost-free
Shelf life 24 months In unopened original packaging
Technical properties

After-processing / operating properties

Supplier-published operating and bath-control conditions for immersion cleaning with BONDERITE® C-AK 5948 R EU AERO.

Property Value Unit Method / condition
Working concentration 5–25 % v/v Diluted in water; selected according to soil level
Operating temperature 65–80 °C Immersion cleaning
Contact time 5–15 minutes Immersion cleaning
Ultrasonic compatibility Suitable — Supplier identifies product as ideal for ultrasonic tanks
Bath-control endpoint 5.2 pH Titrate 100 mL bath sample with 1.0 N sulfuric acid
Bath concentration calculation V × 17.8 mL/L V = mL of 1.0 N H₂SO₄ used to reach pH 5.2