BONDERITE C-AK 4338LP2

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 4338LP2

Main features

  • High-Temperature Oxide-Scale Conditioning
  • Equal-Volume Two-Liquid Mixing
  • 15 to 25% Component Concentration

Product Description

BONDERITE® C-AK 4338L AERO is a two-component alkaline permanganate scale remover and conditioner developed specifically for jet-engine cleaning. It chemically modifies high-temperature oxide scale on ferrous and heat-resistant alloys, conditioning the deposit for easier chemical removal in subsequent processing steps. Supplied as two liquid concentrates, the system supports safer and easier handling than powdered products, offers a wide operating-concentration range, and can be used in mild-steel tanks.

Key features

  • Jet-engine scale conditioning: Developed to modify high-temperature oxide deposits before subsequent chemical removal.
  • Two-component liquid system: Supplied as liquid Part A and Part B concentrates for tank make-up and maintenance.
  • Ferrous and heat-resistant alloy compatibility: Suitable for ferrous and high-temperature alloys under controlled process conditions.
  • Flexible bath concentration: May be operated across a range of concentrations to address different scale types.
  • Long bath life: Identified by the supplier as supporting extended bath operation.

Applications / Suitable for

  • Jet-engine cleaning processes
  • Conditioning of high-temperature heat scale
  • Ferrous alloys
  • High-temperature and heat-resistant alloys
  • Immersion metal-pretreatment systems
Product Family

BONDERITE C-AK 4338LP2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
Optimum 19–24°C (protect from freezing) °C
General Properties
Appearance
Dark violet liquid
Specific Gravity
Not Published

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published product characteristics and storage information for BONDERITE® C-AK 4338L AERO.

Property Value Unit Method / condition
Technology Metal pretreatment — Supplier classification
Chemical type Permanganate scale remover / conditioner — Supplier classification
Components Two-component — Part A and Part B liquid concentrates
Part A appearance Colorless — As supplied
Part B appearance Dark violet — As supplied
Optimal storage temperature 19–24 °C Store unopened in a dry location
Adverse storage limits Below 12 or above 38 °C May adversely affect product properties
Freezing sensitivity Protect from freezing — Storage requirement
Technical properties

After-processing / operating properties

Supplier-published bath preparation, operating, and control conditions for BONDERITE® C-AK 4338L AERO.

Property Value Unit Method / condition
Part A concentration 15–25 % v/v Final working solution
Part B concentration 15–25 % v/v Use Part A and Part B in equal volumes
Make-up heating temperature 90 °C Heat while mixing during solution preparation
Operating temperature 80–95 °C Immersion scale-conditioning step
Immersion time 30–60 minutes Scale-conditioning step in the published multi-stage process
Part 1 bath-control calculation [(2 × A) − B] × 1.05 % v/v 5 mL sample; titrate with 1.0 N H₂SO₄ to pH 8.3 and then pH 4.0
Part 2 bath-control calculation V × N × 21.8 % v/v Titrating Solution 1565; V = mL used and N = solution normality
Compatible process-tank material Mild steel — Supplier-published equipment compatibility

Leading Brands Trust in Our Products and Services