Main features

  • Two-Part Alkaline-Permanganate System Component
  • Jet-Engine Heat-Scale Conditioning
  • Liquid-Concentrate Bath Make-Up

Product Description

BONDERITE® C-AK 4338L AERO (Part 1) is the Part 1 component of a two-component alkaline permanganate scale remover and conditioner developed specifically for jet engine cleaning. Used together with BONDERITE® C-AK 4338L AERO Part 2, it chemically modifies high-temperature oxide scale on ferrous and heat-resistant alloys to condition deposits for efficient removal during subsequent chemical processing. The liquid concentrate is supplied for safer handling than powdered products and is suitable for both bath make-up and bath maintenance.

Key Features

  • Part of a two-component conditioning system for high-temperature oxide scale removal.
  • Developed for jet engine cleaning and metal pretreatment operations.
  • Suitable for ferrous and heat-resistant alloys under controlled process conditions.
  • Liquid concentrate for safer handling and easier bath preparation than powdered alternatives.
  • Long bath life with supplier-stated REACH compliance.

Applications / Suitable for

  • Jet engine cleaning
  • High-temperature oxide scale conditioning
  • Ferrous alloys
  • Heat-resistant alloys
  • Metal pretreatment processes
  • Immersion processing as part of the BONDERITE® C-AK 4338L AERO system
Product Family

BONDERITE C-AK 4338LP1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
Optimum 19–24°C (protect from freezing) °C
General Properties
Appearance
Colorless liquid
Specific Gravity
Not Published

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Chemical type Permanganate scale remover / conditioner — Supplier classification
Component Part 1 of two-component system — Used with Part 2 in equal volumes
Appearance Colorless — Part 1 as supplied
Application Metal pretreatment — Supplier classification
Specific benefit Long bath life — Supplier feature
Alloy compatibility Ferrous and heat-resistant alloys — Do not use on reactive alloys such as aluminum
Optimal storage 19–24 °C Protect from freezing
Technical Properties

After-Processing / Operating Properties

Property Value Unit Method / Condition
Part 1 working concentration 15–25 % by volume Final working solution
Mix ratio Equal volume with Part 2 — Part 1 added to water before Part 2
Solution preparation temperature 90 °C Heat while mixing
Operating temperature 80–95 °C Immersion scale-conditioning step
Immersion time 30–60 minutes Published process sequence
Bath concentration calculation [(2 × A) − B] × 1.05 % by volume Part 1 titration using 1.0 N sulfuric acid
Compatible tank material Mild steel — Supplier recommendation