BONDERITE C-AK 298

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 298

Main features

  • Non-Silicated Aluminum Immersion Cleaner
  • Multi-Soil Removal and Free Rinsing
  • 54 to 82 deg C Immersion Cleaning

Product Description

BONDERITE® C-AK 298 is a non-silicated alkaline immersion cleaner formulated for cleaning aluminum and aluminum alloys prior to anodizing and chemical conversion coating. The free-rinsing liquid formulation removes soils, oils, greases, inks, and wax-based markings while preparing aluminum surfaces for subsequent finishing operations. It is designed for high-temperature immersion cleaning in metal processing and fabrication applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Non-silicated alkaline cleaner formulated for aluminum and aluminum alloys.
  • Free-rinsing immersion cleaner that prepares surfaces for anodizing and conversion coating.
  • High-temperature operation for effective removal of oils, greases, inks, soils, and wax-based markings.
  • Liquid concentrate designed for immersion cleaning processes.

Applications / Suitable for

  • Cleaning aluminum and aluminum alloys
  • Surface preparation before anodizing
  • Surface preparation before chemical conversion coating
  • High-temperature immersion cleaning
  • Metal pretreatment operations
Product Family

BONDERITE C-AK 298

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
Appearance
Brown liquid
Specific Gravity
Not Published

Additional Information

Property Value Unit Method / Condition
Technology Industrial Cleaner — Supplier classification
Product type Alkaline immersion cleaner — Supplier classification
Physical state Liquid — As supplied
Color Brown — As supplied
Chemistry Non-silicated alkaline formulation — Supplier description
Property Value Unit Method / Condition
Application method Immersion — Supplier recommendation
Working concentration 8.2–18.6 mL/L Supplier operating range
Operating temperature 54–82 (130–180) °C (°F) High-temperature immersion cleaning
Treatment time 3–15 minutes Supplier operating range
Surface condition after cleaning Free-rinsing, prepared for anodizing or conversion coating — Supplier application guidance