BONDERITE C-AD 4215

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AD 4215

Main features

Product Description

BONDERITE® C-AD 4215 AERO is a clear, colorless liquid additive formulated to enhance the cleaning performance of BONDERITE® C-AK 4215 AERO and other alkaline cleaners when difficult-to-remove soils are encountered. Suitable for both spray and immersion cleaning systems, the additive readily dissolves into alkaline cleaning baths, is compatible with ferrous and nonferrous alloys when used with a compatible base cleaner, and rinses cleanly from treated parts with cool to warm water.

Key Features

  • Cleaning-performance enhancer for BONDERITE® C-AK 4215 AERO and other compatible alkaline cleaners.
  • Low addition rate of only 1–2% by volume minimizes changes to existing cleaning processes.
  • Suitable for spray and immersion systems with recommended air or mechanical agitation for immersion cleaning.
  • Compatible with ferrous and nonferrous alloys when the selected alkaline cleaner is also compatible.
  • Readily soluble and free-rinsing for efficient incorporation into alkaline cleaning baths.

Applications / Suitable for

  • Enhancing alkaline cleaner performance
  • Spray alkaline cleaning systems
  • Immersion alkaline cleaning systems
  • Cleaning difficult-to-remove soils
  • Ferrous alloy cleaning processes
  • Nonferrous alloy cleaning processes
Product Family

BONDERITE C-AD 4215

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
0–40°C °C
General Properties
Appearance
Clear, colorless liquid
Specific Gravity
Density: 0.951–0.961 g/mL

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Supplier-published characteristics of BONDERITE® C-AD 4215 AERO.

Property Value Unit Method / Condition
Technology Metal Pretreatment — Supplier classification
Product Type Additive — Supplier classification
Application Immersion and Spray — Supplier classification
Appearance Clear, colorless liquid — As supplied
Density 0.951–0.961 g/mL Typical property
Flash Point 110 °C Cleveland Open Cup Method
Storage Temperature 0–40 °C Recommended storage
Shelf Life 24 months Original unopened packaging
Technical Properties

After-Processing / Operating Properties

Supplier-recommended operating conditions when using BONDERITE® C-AD 4215 AERO with compatible alkaline cleaners.

Property Value Unit Method / Condition
Recommended addition level 1–2 % by volume Add after alkaline cleaner is fully mixed
Operating temperature 60–80 °C Preferred operating range
Preferred operating temperature 70 °C Supplier recommendation
Application methods Spray and immersion — Compatible alkaline cleaning systems
Immersion agitation Air or mechanical agitation recommended — Immersion cleaning
Rinsing Cool to warm water rinse — Follow rinsing procedure of the selected alkaline cleaner
Compatibility Ferrous and nonferrous alloys — Provided the base cleaner is compatible with the substrate