BIOACT 280E

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT 280E

Main features

  • High-Melting Wax Removal
  • Multi-Polymer Cleaning Compatibility
  • Low-Odor Low-Volatility Cleaning

Product Description

BIOACT® 280E Precision Cleaner is a USDA Certified Biobased semi-aqueous cleaner formulated from a blend of aliphatic esters and surface-active agents. It is designed to dissolve paraffinic, microcrystalline, plating, and thermoplastic fixturing waxes while also removing pitches, greases, buffing compounds, metalworking fluids, coolants, hydraulic fluids, and lubricating oils. The low-odor cleaner is suitable for heated immersion cleaning and is compatible with many polymeric substrates, elastomers, and ferrous and non-ferrous alloys.

Key features

  • High-melting soil removal: Dissolves paraffinic, microcrystalline, plating, and thermoplastic fixturing waxes.
  • Broad material compatibility: Suitable for many polymeric substrates, elastomers, and ferrous and non-ferrous alloys.
  • High wax-loading capacity: Supports wax loading levels of up to 40%.
  • Low-volatility formulation: Provides very low odor, a vapor pressure below 0.002 mmHg at 20°C, and a flash point of 285°F (141°C).

Applications / Suitable for

  • Removal of paraffinic, microcrystalline, plating, and fixturing waxes
  • Removal of pitches, greases, coolants, hydraulic fluids, polishing compounds, buffing compounds, metalworking fluids, and lubricating oils
  • Heated immersion cleaning processes
  • Replacement of selected vapor-degreasing solvents and hot-oil dewaxing processes
Product Family

BIOACT 280E

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

Thermal Properties
Flash Point
141 °C
General Properties
Vapor Pressure
<0.002 mmHg
Physical Properties
Viscosity
7.3 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and process properties. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product type Semi-aqueous precision cleaner based on aliphatic esters and surface-active agents — As supplied
Odor Very low — Typical value
Flash point 285 (141) °F (°C) Typical value
Specific gravity 0.86 — At 25°C
Vapor pressure <0.002 mmHg At 20°C
Viscosity 7.3 cPs At 25°C
Kauri-butanol value 90 — Typical value
Volatile organic compound content 70 g/L Reported in the supplied TDS
Recommended wash-bath concentration 100 % Heated immersion cleaning
Recommended wash-bath temperature 190–205 (88–96) °F (°C) Heated immersion cleaning
Recommended DI-water rinse temperature 190–205 (88–96) °F (°C) Following heated immersion cleaning
Shelf life 36 months Original sealed container stored above 50°F (10°C); protect from freezing