BECTRON PL 4122-37

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BECTRON PL4122-37

Main features

  • Transparent Urethane-Alkyd Conformal Coating
  • 30-Minute 80 deg C Cure
  • 1 x 10^15 ohm-cm Volume Resistivity

Product Description

Bectron® PL 4122-37 E BLF FLZ is a transparent urethane-modified alkyd conformal coating for protecting printed circuit boards and electronic components. The low-viscosity varnish is formulated for room-temperature or oven curing and supports select-coat, spray, automated dipping, brushing, and hand-spray processes. The cured thin film retains flexibility and documented dielectric properties under environmental exposure. Supported applications include electronics used in automotive, marine-navigation, industrial, and corrosive-gas environments, together with hybrids, surface-mount devices, and discrete components. The 37% solids grade is intended for general coating applications.

Key features

  • 37% solids grade: The PL 4122-37 grade has a non-volatile content of 37 ± 1% under ISO 3251 conditions.
  • Flexible cure options: Documented cure schedules include 16 hours at 23°C or 30 minutes at 80°C.
  • Thin-film electrical properties: Typical cured data include 1 × 10¹⁵ ohm·cm volume resistivity and CTI 600.

Applications / Suitable for

  • Printed circuit boards exposed to automotive, marine-navigation, industrial, or corrosive-gas environments
  • Hybrid electronic assemblies
  • Surface-mount devices and discrete components
Product Family

BECTRON PL 4122-37

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature Resistance
134 ˚C
Electrical Properties
Dielectric Strength
112 kV/mm
Permittivity
3.5 F/m
Chemical Properties
Water Absorption
1.5 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Non-volatile content 37 ± 1 % ISO 3251; 1.5 g, 2 h at 130°C
Flow time 40 ± 3 s DIN EN ISO 2431, 4 mm cup at 23°C
Approximate viscosity 50 mPa·s Associated with 4 mm cup flow time
Density 0.86 ± 0.01 g/cm³ DIN EN ISO 2811-2 at 23°C
Shelf life 6 months At 23°C
Dust-dry time 0.25 h At 23°C
Touch-dry time 1 h At 23°C
Cure options 16 h at 23°C; 0.5 h at 80°C N/A Air cure or batch-oven cure
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Service temperature -50 to 105 °C Documented range
Shrinkage 16 % CQP014-1
Heat-aging weight loss 11 % ASTM C792
Staining No staining N/A ASTM D925 on common substrates