AXSON EC-433-2

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

AXSON EC-433-2

Main features

  • Up to 300 deg F Continuous Tooling
  • Up to 350 deg F Intermittent Exposure
  • Aluminum-Filled Tooling Formulation

Product Description

AXSON EC-433-2 is the fast-hardener configuration of the EC-433 aluminum-filled epoxy casting system developed for heat-resistant cast tooling. The room-temperature-hardening system provides a 120-minute work life at 77°F (25°C), accepts additional bulk aluminum filler, and requires a controlled heat cure for service above 150°F (66°C). Properly cured tools can operate continuously at temperatures up to 300°F (160°C) and intermittently up to 350°F (177°C).

Key features

  • High-temperature tooling performance: Supports continuous tool temperatures up to 300°F (160°C) and intermittent temperatures up to 350°F (177°C) after the required cure.
  • Fast hardener configuration: Provides a 120-minute work life at 77°F (25°C) for comparatively faster processing within the EC-433 system.
  • Dimensional stability: The aluminum-filled epoxy formulation exhibits low linear shrinkage and can accept additional N-20 aluminum grain.
  • Room-temperature B-stage cure: Develops initial hardness at room temperature before the required controlled heat-cure schedule.

Applications / Suitable for

  • Vacuum-form molds
  • Compression molds
  • Prototype injection molds
  • RIM molds
  • Foam molds and other high-temperature cast-tooling applications
Product Family

AXSON EC-433-2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
gray resin / amber hardener
Mix Ratio
100R/12H
Pot Life
2 hours
Specific Gravity
1.62

Additional Information

Technical properties

As-supplied / before-processing properties

Typical handling and processing properties for EC-433-2 at 77°F (25°C), unless otherwise stated.

Property Value Unit Method / condition
Product type Aluminum-filled epoxy casting system — EC-433 resin with EC-433-2 fast hardener
Color Gray resin / amber hardener — As supplied
Mix ratio, resin:hardener 100R:12H parts by weight EC-433-2 fast configuration
Specific gravity 1.62 g/cc Mixed system at 77°F (25°C)
Mixed density 0.058 lb/cu. in. At 77°F (25°C)
Mixed viscosity 9,000 cps At 77°F (25°C)
Work life 120 minutes At 77°F (25°C)
Demold time 24 hours See recommended cure schedule
Maximum casting thickness <1 in. Without aluminum-filler additive
Suggested casting mass <2 cu. ft. With N-20 aluminum bulk-filler additive
Bulk-filler mix ratio 100:155 parts by weight Catalyzed EC-433:N-20 aluminum grain
Preliminary cure 24 hours at 77°F (25°C) + 3 hours at 150°F (66°C) — Minimum cure schedule; cool before demolding
Recommended post cure 2 hours at 200°F (93°C) + 2 hours at 250°F (121°C) + 2 hours at 300°F (149°C) — When additional post cure is required
Shelf life — resin 12 months Original unopened container at 47–77°F (8–25°C)
Shelf life — hardener 24 months Original unopened container at 60–77°F (15–25°C)
Technical properties

After-processing / final-state properties

Typical cured properties for EC-433-2 measured on a 5 × ½ × ½-inch cast bar, unless otherwise stated.

Property Value Unit Method / condition
Continuous operating temperature 300 (160) °F (°C) Properly post-cured tool
Intermittent operating temperature 350 (177) °F (°C) Properly post-cured tool
Tensile strength 5,750 (40) psi (MPa) ASTM D638-91
Tensile modulus 941,200 (6,489) psi (MPa) ASTM D638-91
Flexural strength 10,620 (73) psi (MPa) ASTM D790-92
Flexural modulus 700,900 (4,833) psi (MPa) ASTM D790-92
Compressive strength 16,300 (112) psi (MPa) ASTM D695-91
Notched Izod impact strength 11.8 in-lbf/in. ASTM D256-93A
Coefficient of thermal expansion 28 (51) ppm/°F (ppm/°C) TMA
Glass transition temperature, Tg 288 (142) °F (°C) DMA
Hardness 90 Shore D Typical cured property
Linear shrinkage 0.005 in./in. 200 cm³ mold, EC-433-2
Linear shrinkage with N-20 aluminum grain 0.002 in./in. 4,650 cm³ mold

Leading Brands Trust in Our Products and Services