AXAREL 9100

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

AXAREL 9100

Main features

  • 96 deg C Flash Point
  • Multi-Soil Cleaning Removal
  • Polymer/Elastomer and Multi-Metal Compatibility

Product Description

AXAREL™ 9100 Solvent Cleaner is a high-flash-point solvent cleaner for manual and immersion cleaning processes. Its broad-based solvency removes mineral and synthetic oils, lubricants, coolants, greases, waxes, rust inhibitors, fingerprint oils, dust, and particulate matter. The cleaner is compatible with many polymeric substrates and elastomers and is suitable for use with ferrous and non-ferrous alloys. A low vapor pressure and low non-volatile residue support controlled cleaning and surface preparation, while the 96 °C (205 °F) flash point permits evaluation for elevated-temperature immersion cleaning.

Key features

  • High flash point: Provides a flash point of 96 °C (205 °F) for manual and elevated-temperature immersion cleaning processes.
  • Broad soil removal: Removes oils, lubricants, coolants, greases, waxes, rust inhibitors, fingerprint oils, dust, and particulate matter.
  • Material compatibility: Compatible with many polymeric substrates and elastomers and suitable for ferrous and non-ferrous alloys.

Applications / Suitable for

  • Manual cleaning by brush, pad, or cloth
  • Immersion cleaning
  • Spray-under-immersion cleaning systems
  • Surface preparation and removal of industrial soils
Product Family

AXAREL 9100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
96 °C
General Properties
Specific Gravity
0.83
Vapor Pressure
0.18 mmHg
Physical Properties
Viscosity
2.2 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical properties of AXAREL™ 9100 as supplied. Typical property data are not intended for specification purposes.

Property Value Unit Method / condition
Odor Essentially odorless — Typical
Flash point 205 (96) °F (°C) Typical
Specific gravity 0.83 — At 25 °C
Viscosity 2.2 cP At 25 °C
Kauri-butanol value 39 — Typical solvency value
Vapor pressure 0.18 mm Hg At 20 °C
Distillation range 430–563 (221–295) °F (°C) Typical
Non-volatile residue 40 ppm Typical