ARATHANE 7762-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARATHANE 7762-1

Main features

  • Controlled 5 mil Bondline
  • Two-Hour Working Life
  • Automated Non-Slump Dispensing

Product Description

ARATHANE 7762-1 Thermal Transfer Adhesive is a pink, one-component polyurethane paste for thermally conductive attachment of components on printed wiring boards. A controlled 5 mil bondline supports repeatable assembly of flat packs, PLCCs, and other devices where adhesive thickness affects placement and heat transfer. Its thixotropic, non-slump consistency enables automatic dispensing, while a working life of at least two hours at 23 deg C supports production use. After cure, the adhesive provides 0.80 W/m-K thermal conductivity, 600 to 660 V/mil dielectric strength, and substrate-specific lap-shear performance. The 100% solids, solvent-free formulation also supports bonding, filleting, and component protection.

Key Features

  • Controlled 5 mil bondline: Supports repeatable component placement and adhesive thickness.
  • Two-hour working life: Provides at least two hours of working time at 23 deg C.
  • Automated non-slump dispensing: Thixotropic rheology supports controlled, reduced-handling application.

Applications

Bonding, filleting, and protection of flat packs, PLCCs, and other components on printed wiring boards.

Product Family

ARATHANE 7762-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
pink paste
Density (g)
1.9-2.3 g/cm3
Pot Life
2 hours
Physical Properties
Viscosity
300,000 - 600,000 mPa.s
Thermal Properties
Flash Point
94 °C
Glass Transition Temperature (Tg)
-63 °C
Operating Temperature
115 °C
Thermal Conductivity
0.80 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

One-component adhesive values; storage and test conditions are shown with each property.

PropertyValueUnitMethod / condition
AppearancePink paste-Visual
Density2.0 to 2.3g/cm3ASTM D-792
Viscosity300,000 to 500,000cPASTM D-2393 at 25 deg C
Flash point>94deg CASTM D93
Solids100%ASTM D2369
Working life>=2h23 deg C
Shelf life3monthsSealed original container below -40 deg C; from shipment
Technical properties

After-processing / final-state properties

Cured-material values; mechanical results apply only to the stated ASTM D1002 substrates and conditions.

PropertyValueUnitMethod / condition
Hardness65 to 90Shore ATypical cured value
Glass-transition temperature-63deg CISO 11359
Thermal conductivity0.80W/m-KISO 8894/90
Dielectric strength600 to 660V/milIEC 60243
Volume resistivity2.9 x 10^14ohm-cmIEC 60093
Lap-shear strength270psiASTM D1002 at 25 deg C; aluminum
Lap-shear strength300psiASTM D1002 at 25 deg C; Ajax-scrubbed nickel plate
OutgassingTML 0.28; CVCM 0.03%ASTM E595 at 10^-6 Torr