ARATHANE 5753LV

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ARATHANE 5753

Main features

  • Low-Viscosity Casting Flow
  • Controlled Two-Part Processing
  • Stress-Sensitive Electronics Encapsulation

Product Description

ARATHANE 5753 A/B (LV) Casting Compound is a low-viscosity, two-component polyurethane liquid for casting and encapsulating electrical and electronic assemblies. The A/B (LV) system is mixed and cured as a complete formulation, providing flow around coils, trimpots, potentiometers, modules, and other stress-sensitive devices. Its liquid processing format supports placement before cure, while the cured system supplies the hardness, electrical insulation, and thermal characteristics required for protective encapsulation. Part A and Part B remain distinct handling components and must be combined at the specified ratio and cure schedule to obtain the intended material.

Key Features

  • Low-viscosity casting flow: Supports casting and encapsulation around electrical and electronic components.
  • Controlled two-part processing: The A/B components cure together to form the intended encapsulant.
  • Stress-sensitive assembly use: Suited to coils, trimpots, potentiometers, modules, and similar devices.

Applications

Encapsulation of coils, trimpots, potentiometers, modules, and stress-sensitive electrical or electronic assemblies.

Product Family

ARATHANE 5753LV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
70,000 mPa.s
General Properties
Appearance
amber liquid
Specific Gravity
1.16-1.26
Thermal Properties
Flash Point
177 °C