ARALDITE MY721

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE MY721

Main features

  • Low-Viscosity Reinforcement Wet-Out
  • Long Processing Pot Life
  • High-Temperature Composite Performance

Product Description

ARALDITE MY 721 Epoxy Resin is a clear brown liquid tetrafunctional glycidylamine resin component for high-temperature composite systems. Typical viscosity is 3,000 to 6,000 cP at 50 deg C, with density of 1.15 to 1.18 g/cm^3 at 25 deg C, providing a low-viscosity processing profile for reinforcement wet-out. Used with ARADUR 5200, the resin supports filament winding with long pot life at processing temperatures and high glass-transition temperatures after the specified cure. Applications include aerospace, spacecraft, high-performance composite parts, and industrial composites. Final mechanical and thermal properties remain tied to the selected hardener, formulation, specimen, and cure schedule.

Key features

  • Low-viscosity processing profile: Typical viscosity is 3,000 to 6,000 cP at 50 deg C for reinforcement wet-out.
  • Long processing pot life: The MY 721/ARADUR 5200 system provides extended working time at processing temperatures.
  • High-temperature composite system: The specified formulation develops high glass-transition temperatures after cure.

Applications

Filament winding for aerospace, spacecraft, high-performance composite parts, and industrial composites in specified MY 721 systems.

Product Family

ARALDITE MY721

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
clear brown liquid
Density (g)
1.15-1.18 g/cm3
Mix Ratio
100:35 by weight
Physical Properties
Viscosity
3,000-6,000 mPa.s
Electrical Properties
Dielectric Strength
17.32 kV/mm
Surface Resistivity
7.4 x 10^16 Ohms/sq
Volume Resistivity
1.1 x 10^16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical MY 721 resin-component data.

PropertyValueUnitMethod / condition
AppearanceClear brown liquid-As supplied
Density1.15 to 1.18g/cm^325 deg C
Viscosity3,000 to 6,000cP50 deg C
Epoxy equivalent weight111 to 117g/eqProduct value range