ARALDITE GY6010

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE GY6010

Main features

  • Medium-Viscosity Liquid Processing
  • Multiple Hardener Cure Options
  • Versatile Resin Formulation Base

Product Description

ARALDITE GY 6010 Epoxy Resin is a medium-viscosity, unmodified liquid bisphenol-A epoxy resin for room-temperature and heat-cured systems. Its typical as-supplied profile includes 11,000 to 13,000 mPa s viscosity at 25 deg C, an epoxy equivalent of 182 to 192 g/eq, and density of 1.15 to 1.18 g/cm^3. The resin can be cured with multiple hardener types and formulated with compatible fillers, diluents, and accelerators. This versatility supports coatings, matrix-resin applications, electrical systems, adhesives, and civil-engineering work. Processing and final performance depend on the selected hardener, ratio, and cure schedule, so formulation data remain tied to the stated combination and test conditions.

Key features

  • Medium-viscosity liquid handling: Typical viscosity is 11,000 to 13,000 mPa s at 25 deg C.
  • Flexible cure formulation: The resin can be combined with multiple hardener types for room-temperature or heat-cured systems.
  • Compatible formulation base: Documented compatibility includes many fillers, diluents, and accelerators.

Applications

Coatings, matrix resins, electrical systems, adhesives, and civil-engineering formulations.

Product Family

ARALDITE GY6010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
clear, slight haze
Density (g)
1.15-1.18 g/cm3
Physical Properties
Viscosity
11,000-14,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical ARALDITE GY 6010 resin values from the exact-grade technical data sheet.

PropertyValueUnitMethod / condition
AppearanceClear, no contamination-Visual; typical
Color1 maximumGardnerTypical
Epoxy value5.2 to 5.5eq/kgTypical
Epoxy equivalent182 to 192g/eqTypical
Viscosity11,000 to 13,000mPa s (cP)25 deg C; typical
Density1.15 to 1.18 (9.6 to 9.8)g/cm^3 (lb/gal)25 deg C; typical
Flash point254 (490)deg C (deg F)Closed cup; typical
Technical properties

After-processing / final-state properties

Values apply only to 100 parts by weight ARALDITE GY 6010 with 50 parts ARADUR 2964. Cure and conditioning are preserved for each result.

PropertyValueUnitMethod / condition
TransparencyClear-GY 6010/ARADUR 2964 formulation
Surface appearanceSmooth, glossy-GY 6010/ARADUR 2964 formulation
ExudationNone-GY 6010/ARADUR 2964 formulation
Impact test70in-lbAfter 2 months at 20 deg C and at 60 deg C
Mandrel test180 at 20 deg C; 60 at 60 deg Cdeg15 mm mandrel; after 2 months
Adhesion after boiling-water exposureUnchanged-Sandblasted mild-steel sheet; 6 hours at 96 deg C

Leading Brands Trust in Our Products and Services