HUNTSMAN ARALDITE CW 1446

Harmonization Code : 3909509090 | Polyurethanes potting

HUNTSMAN ARALDITE CW 1446

Main features

  • Filled, Solvent-Free Epoxy Casting and Impregnation System
  • Six-Hour Cure Cycle
  • UL 94 V-0 Classification

Product Description

ARALDITE® CW 1446 / ARADUR® HY 2919-1 Epoxy System is a filled, solvent-free two-part epoxy casting and impregnation system for electrical and electronic components. The mineral-filled resin combines with a low-viscosity anhydride hardener to support impregnation where dielectric properties and thermal-shock resistance are required. The system is documented for power diodes, rectifiers, power transistors, transformers, and capacitors. A typical resin-to-hardener ratio of 100:24 by weight and a six-hour cure at 100°C are listed for the combined system, with final properties reported for the cured material.

Key features

  • Casting and impregnation system: The filled epoxy resin and low-viscosity anhydride hardener support electrical component processing.
  • Dielectric cured property: Typical cured dielectric strength is 25 kV/mm.
  • Thermal and flame properties: Typical thermal conductivity is 0.67 W/m·K with UL 94 V-0 classification at 10 mm.

Applications / Suitable for

  • Power diodes and rectifiers
  • Power transistors
  • Transformers and capacitors
Product Family

ARALDITE CW 1446

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Grey-brown, viscous liquid / Yellow brown ro red brown clear liquid
Component System
Resin / Hardener
Mix Ratio
100:24
Pot Life
525 minutes
Specific Gravity
1.75 – 1.83 / 1.180 – 1.220

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin appearance Gray-brown filled epoxy N/A ARALDITE CW 1446 BDF
Resin viscosity 15,000 to 30,000 mPa·s As supplied
Resin density 1.75 to 1.83 g/cm³ As supplied
Hardener appearance Brown anhydride liquid N/A ARADUR HY 2919-1
Hardener viscosity 50 to 100 mPa·s As supplied
Hardener density 1.18 to 1.22 g/cm³ As supplied
Mix ratio 100:24 parts by weight Resin : hardener
Technical properties

After-processing / final-state properties

Typical final-state values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Reference cure 6 h At 100°C
Hardness 92 Shore D Typical cured value
Dielectric strength 25 kV/mm Typical cured value
Thermal conductivity 0.67 W/m·K Typical cured value
Service temperature range -40 to 181 °C Documented system range
Flammability classification V-0 UL 94 At 10 mm thickness