ARALDITE CW 1302

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE CW1302

Main features

  • Thermally Conductive Thermal Interface
  • Low Water Absorption
  • Good Long-Term Thermal Resistance

Product Description

ARALDITE® CW 1302 GB is a highly filled epoxy casting resin designed for electrical insulation and encapsulation applications. When used within its recommended casting resin system, it can be processed and cured at room temperature or moderately elevated temperatures. The material offers good thermal conductivity, low water absorption, long-term thermal resistance, and UL 94 V-0 flammability performance at 3.2 mm thickness. It is suitable for the manufacture of inductive components, wound capacitors, and electrical devices operating in potentially explosive environments while providing reliable dielectric and mechanical performance in demanding electrical insulation applications.

Key features

  • Electrical insulation performance: High volume resistivity, dielectric strength of 15 kV/mm, and CTI greater than 600 support demanding electrical insulation applications.
  • Thermally conductive filled system: Thermal conductivity of 0.83 W/m·K and a Relative Temperature Index of 181°C support thermal management and long-term service performance.
  • Flame-retardant formulation: Achieves UL 94 V-0 classification at 3.2 mm and complies with EN 50014 and EN 50028 requirements.

Applications / Suitable for

  • Inductive components
  • Wound capacitors
  • Electrical insulation castings
  • Electrical devices operating in potentially explosive environments
  • Encapsulation and protection of electrical assemblies
Product Family

ARALDITE CW 1302

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
40000 mPa.s
General Properties
Filler Content
66 %
Specific Gravity
1.76
Thermal Properties
Flash Point
>200 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Representative processing and material properties for the casting resin system.

Property Value Unit Method / condition
Mix ratio (Araldite Resin to Hardener) 100 : 11 pbw Casting resin system
Viscosity 40,000 mPa·s 25°C
Flash point >200 °C DIN 51 758
Filler content 66 %  
Technical properties

After-processing / final-state properties

Properties determined on standard specimens cured for 24 h at 25°C followed by 6 h at 60°C.

Property Value Unit Method / condition
Thermal conductivity 0.83 W/m·K ISO 8894-1, 18°C
Glass transition temperature 76 °C