ARALDITE AW8680

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE AW8680

Main features

  • Flexible Polyurethane Adhesive Formulation
  • Convenient 1:1 Volume Mixing
  • Fifteen-Minute Mixed Pot Life

Product Description

ARALDITE AW 8680 Resin is a white paste resin component for a flexible two-part polyurethane adhesive system. Published AW 8680 component characteristics include 1.14 specific gravity and 48,000 cP viscosity at 25 deg C. In the AW 8680/HW 8680 configuration, the two parts combine at 93:100 by weight or 1:1 by volume, with a typical 15-minute pot life for a 100 g mass at 25 deg C. This formulation is used for plastic bonding, including polycarbonate and nylon headlamp assemblies, and for primed metal bonding. Its cured profile combines 225% elongation with Shore D 30 hardness under the stated test conditions.

Key features

  • Paste resin consistency: The AW 8680 component has a typical viscosity of 48,000 cP at 25 deg C.
  • Convenient volume mixing: The AW 8680/HW 8680 configuration uses a 1:1 volume ratio.
  • Flexible cured system: The stated formulation reaches typical 225% elongation after cure.

Applications

Plastic bonding, including polycarbonate and nylon headlamp assemblies, and primed metal bonding in the AW 8680/HW 8680 configuration.

Product Family

ARALDITE AW8680

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
3 minutes
Mechanical Properties
Elongation
250 %
Thermal Properties
Glass Transition Temperature (Tg)
30 °C

Additional Information

Technical properties

As-supplied / before-processing properties

AW 8680 resin values are component-specific; mixed values apply only to the AW 8680/HW 8680 configuration.

PropertyValueUnitMethod / condition
AW 8680 appearanceWhite paste-Visual; typical
AW 8680 specific gravity1.14-ASTM D792; 25 deg C; typical
AW 8680 viscosity48,000cPASTM D2393; 25 deg C; typical
System mix ratio93:100 by weight; 100:100 by volumepartsAW 8680 resin to HW 8680 hardener
Mixed pot life15minASTM D2471; 100 g at 25 deg C; typical