ARALDITE AW139

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AW139

Main features

  • Two-Component Room-Temperature Epoxy
  • High-Temperature Chemical Resistance
  • Multi-Material Metal/Composite/Electronics Bonding

Product Description

ARALDITE® AW 139-1 / Hardener HW 5323-1 is a two-component, room-temperature-curing epoxy paste adhesive for structural bonding where elevated temperatures or aggressive service environments may be encountered. The thixotropic, non-sagging mixed adhesive fills gaps up to 5 mm and is suitable for bonding metals, electronic components, GRP structures, and other supported assemblies. A 100:50 mix ratio by weight or volume, approximately 110-minute pot life at 25°C, and specified lap shear strength above 14 MPa at 25°C provide a practical balance of application control and bonded-joint performance.

Key features

  • Environmental resistance: Resistant to water and a wide variety of chemicals.
  • Gap-filling paste: Thixotropic, non-sagging consistency supports gaps up to 5 mm.
  • Controlled working time: Approximately 110-minute pot life for a 100 g mixed mass at 25°C.

Applications / Suitable for

  • Structural bonding of metals
  • Bonding electronic components
  • GRP structures and assemblies exposed to demanding environments
Product Family

ARALDITE AW139

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Beige
Specific Gravity
1.6
Physical Properties
Viscosity (Part A)
65 mPa.s
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
46000000000000000 Ohms/sq
Volume Resistivity
2700000000000000 Ohms⋅cm

Additional Information

Technical properties

Before-mixing properties

Individual component properties before ARALDITE® AW 139-1 and Hardener HW 5323-1 are combined.

Property ARALDITE® AW 139-1 Hardener HW 5323-1
Color and form Beige paste Grey paste
Specific gravity Approx. 1.6 Approx. 1.5
Viscosity at 25°C 50–80 Pa·s Thixotropic
Mix ratio 100 parts AW 139-1 to 50 parts HW 5323-1 by weight or volume
Technical properties

After-mixing properties

Properties of the mixed adhesive before cure.

Property Value Condition
Color and form Grey paste Mixed adhesive
Specific gravity Approx. 1.6 Mixed adhesive
Rheology Thixotropic Non-sagging paste
Pot life 110 minutes 100 g mixed mass at 25°C
Gap-filling capability Up to 5 mm Non-sag application