Main features

  • Controlled Paste-Grade Resin Handling
  • 80-to-100-Minute System Pot Life
  • Multipurpose Metal and Ceramic Bonding

Product Description

ARALDITE AW 134 Epoxy Resin is a white-to-beige paste resin component for a two-part, room-temperature-curing epoxy adhesive system used with ARADUR HY 991. The resin has a typical specific gravity of 1.2 to 1.3 and viscosity of 20 to 40 Pa s. The complete system mixes at 100:30 by weight or 100:40 by volume and provides a typical 80-to-100-minute pot life for 100 g at 25 deg C. When combined with the specified hardener, it forms a solvent-free multipurpose adhesive for bonding metals, ceramics, and other common substrates. Cured-joint properties belong to the complete AW 134/HY 991 formulation and cure.

Key features

  • Paste-grade resin handling: The AW 134 component has a typical viscosity of 20 to 40 Pa s.
  • Extended mixed working window: The AW 134/HY 991 system provides a typical 80-to-100-minute pot life at 25 deg C.
  • Room-temperature epoxy system: The specified resin and hardener form a solvent-free adhesive that cures at room temperature.

Applications

Bonding metals, ceramics, and other common substrates within the specified AW 134/HY 991 adhesive system.

Product Family

ARALDITE AW134

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
white to beige paste
Mix Ratio
100:30 by weight
Specific Gravity
1.2-1.3

Additional Information

Technical properties

As-supplied / before-processing properties

AW 134 component values are separated from mixed AW 134/HY 991 system data.

PropertyValueUnitMethod / condition
AW 134 appearanceWhite to beige paste-Visual; typical
AW 134 specific gravity1.2 to 1.3-Typical
AW 134 viscosity20 to 40Pa sTypical
System mix ratio100:30 by weight; 100:40 by volumepartsAW 134 resin to HY 991 hardener