ARALDITE AW106

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AW106

Main features

  • Multi-Material Epoxy Bonding
  • Long Adhesive Working Time
  • Electrically Insulating Epoxy

Product Description

ARALDITE® AW 106 Resin / Hardener HV 953U is a two-part, multi-purpose epoxy adhesive for bonding metals, ceramics, wood, vulcanized rubber, foams, and plastics. The viscous system has a 100:80 mix ratio by weight and a long working time for manual application by spatula or stiff brush, as well as mechanical mixing and coating equipment. It cures at temperatures from 20°C to 180°C and develops shear and peel strength for bonded assemblies exposed to static or dynamic loading. The cured adhesive is electrically insulating, supporting bonding applications where electrical isolation is also required.

Key features

  • Multi-material bonding: Suitable for metals, ceramics, wood, rubber, foams, and plastics.
  • Long working time: Provides a typical 2-hour pot life for a 4 fl oz mixed mass at 25°C.
  • Electrically insulating: Combines structural bonding performance with dielectric properties.

Applications / Suitable for

  • General-purpose assembly bonding
  • Metal, ceramic, and wood bonding
  • Plastic, foam, and vulcanized-rubber assemblies
  • Bonded assemblies requiring electrical insulation
Product Family

ARALDITE AW106

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
amber
Pot Life
2 hours
Physical Properties
Viscosity (Part A)
1.17 mPa.s
Viscosity (Part B)
0.92 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
63 °C
Thermal Conductivity
0.22 W/m.K
Electrical Properties
Dielectric Strength
400 kV/mm
Surface Resistivity
12000000000000000 Ohms/sq
Volume Resistivity
710000000000000 Ohms⋅cm
Mechanical Properties
Elongation
9 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the separate components and mixed adhesive. Values are not product specifications.

Property Value Unit Method / condition
Resin appearance Creamy, viscous liquid — Visual
Hardener appearance Amber liquid — Visual
Mix ratio 100:80 By weight Resin:hardener
Mix ratio 100:100 By volume Resin:hardener
Mixed viscosity 54,000 cP ASTM D-2393 at 25°C
Pot life 2 Hours 4 fl oz mixed mass at 25°C
Technical properties

After-processing / final-state properties

Typical cured-material values. Performance in a bonded assembly depends on substrate, preparation, bondline, cure schedule, and test conditions.

Property Value Unit Method / condition
Ultimate tensile strength 33 MPa ASTM D-638
Elongation 9 % ASTM D-638
Glass-transition temperature 63 °C DMA, ASTM D-4065
Hardness 80 Shore D ASTM D-2240
Thermal conductivity 0.22 W/m·K Cured adhesive
Dielectric strength 400 V/mil Cured adhesive