Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AV170

Main features

  • Up to 120 deg C Heat Resistance
  • Up to 3 mm Gap Filling
  • Heat-Resistant Gap-Filling Bonding

Product Description

ARALDITE® AV 170 is a thixotropic, single-component epoxy structural adhesive supplied as a paste for heat-cured bonding. It is recommended for a wide range of metals, temperature-resistant plastics and composites, with railway carriage identified as a product end use. The adhesive cures at 140–180°C, fills gaps up to 3 mm, and contains spacers that maintain a minimum 0.05 mm bondline; a 0.05–0.10 mm adhesive layer is recommended for greatest lap shear under the stated process. Published data include specified lap shear above 20 MPa at 80°C, very good peel strength, good chemical resistance and heat resistance to 120°C. The one-component format removes component mixing, while the thixotropic rheology supports controlled placement before assembly and clamping.

Key features

  • One-component thixotropic paste: Applies directly without component mixing and supports controlled placement on prepared joint surfaces.
  • Gap and bondline control: Fills gaps up to 3 mm and contains spacers that maintain a minimum 0.05 mm adhesive layer.
  • Heat-cured structural performance: Cures at 140–180°C, is heat resistant to 120°C, and has specified lap shear strength above 20 MPa at 80°C.

Applications / Suitable for

  • Railway carriage bonding and assembly
  • Structural bonding of a wide variety of metal substrates
  • Bonding temperature-resistant plastics and composite materials
Product Family

ARALDITE AV170

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Specific Gravity
1.175
Thermal Properties
Flash Point
100 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product-form, handling and bondline-control data for the uncured single-component adhesive.

Property Value Unit Method / condition
Physical form Thixotropic paste — As supplied
Specific gravity 1.15–1.20 — As supplied
Flash point >100 °C As supplied
Gap-filling capability Up to 3 mm Product feature
Spacer-controlled minimum bondline 0.05 mm Built-in spacer feature
Recommended adhesive-layer thickness 0.05–0.10 mm Normally provides the greatest lap shear under the stated process
Technical properties

After-processing / final-state properties

Bonded-joint and cured-property values retain the stated cure and test conditions. Typical values are not guaranteed specifications.

Property Value Unit Method / condition
Lap shear strength at 80°C >20 MPa Method A501; specified value
Lap shear strength at 23°C 23–26 MPa Typical; 60 min cure at 140°C
Lap shear strength at 23°C 26–30 MPa Typical; 60 min cure at 160°C
Lap shear strength at 23°C 28–30 MPa Typical; 60 min cure at 180°C
Roller peel 5.8 N/mm Typical; 30 min cure at 150°C
Roller peel 6.6 N/mm Typical; 30 min cure at 180°C
Glass transition temperature 129 °C Typical; DMA; 2 h cure at 150°C
Lap shear after thermal cycling 26.6 MPa Typical; 100 cycles of 6 h from −30°C to 70°C; 60 min cure at 150°C; test at 23°C