ARALDITE AV 8503

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AV 8503

Main features

  • One-Minute Fixturing Time
  • Heat-Resistant Bonding Service
  • 1:1 Controlled Mixing

Product Description

ARALDITE® AV 8503 Resin / Hardener HV 8503 is a two-component epoxy adhesive paste developed for bonding sheet molding compound, plastics, and metals. The blue resin and beige hardener mix at a convenient 1:1 ratio by volume and form a non-sag paste with approximately 100 minutes of pot life at 25°C. The adhesive combines good flexibility with heat resistance and can achieve rapid handling strength using a heated fixture. Its surface-preparation requirements are limited to a dry wipe before bonding, supporting straightforward assembly processes where controlled paste application and accelerated heat cure are required.

Key features

  • Rapid heat fixture: Reaches fixture strength in approximately one minute on a fixture heated to 116°C.
  • Flexible cured epoxy: Provides 15% elongation with a Shore D hardness of 78.
  • Convenient paste mixing: Uses a 1:1 mix ratio by volume with good weldability and non-sag application behavior.

Applications / Suitable for

  • Sheet molding compound bonding
  • Plastic assembly
  • Metal bonding
Product Family

ARALDITE AV 8503

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
blue
Pot Life
30 minutes
Specific Gravity
1.32
Physical Properties
Viscosity (Part A)
172000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
103 °C
Mechanical Properties
Elongation
15 %