ARALDITE 2011

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 2011

Main features

  • Rubber-to-Wood Epoxy Bonding
  • 2-Hour Working Window
  • 30.4 MPa Aluminum Lap Shear

Product Description

ARALDITE® 2011-A/B is a two-component, multi-purpose epoxy adhesive for bonding metals, ceramics, wood, vulcanized rubber, foams and plastics. The viscous system mixes at 100:80 by weight or 1:1 by volume and provides a typical 2-hour pot life at 25°C for a 4 fl oz mass. It can be applied manually or with meter/mix equipment and cures from 20°C to 180°C without releasing volatile constituents. The cured adhesive is electrically insulating and combines shear and peel performance with resistance to static and dynamic loading. Recommended bondline thickness is 0.05 to 0.10 mm, with handling strength achievable from 12 hours at 20°C to 4 minutes at 150°C under the stated cure schedules.

Key features

  • Broad substrate range: Listed for bonding metals, ceramics, wood, vulcanized rubber, foams and plastics.
  • Extended working time and flexible cure: Typical pot life is 2 hours at 25°C for a 4 fl oz mass, with room-temperature and accelerated heat-cure schedules.
  • Documented bonded-joint performance: Typical aluminum lap shear reaches 30.4 MPa after a 150°C cure for 10-20 minutes, with roller peel of 4.9 N/mm under the stated test conditions.

Applications / Suitable for

  • Metal bonding
  • Ceramic bonding
  • Wood bonding
  • Vulcanized rubber bonding
  • Foam bonding
  • Plastic bonding
Product Family

ARALDITE 2011

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.17
Physical Properties
Viscosity (Part A)
50000 mPa.s
Viscosity (Part B)
35000 mPa.s
Mechanical Properties
Elongation
9 %
Thermal Properties
Glass Transition Temperature (Tg)
63 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the resin, hardener and mixed adhesive. Values are not presented as guaranteed specifications.

Property Value Unit Method / condition
Resin appearance Creamy, viscous liquid — Visual; as supplied
Hardener appearance Amber liquid — Visual; as supplied
Specific gravity Resin 1.17; hardener 0.92 — ASTM D-792; 25°C
Viscosity Resin 50,000; hardener 35,000 cP ASTM D-2393; 25°C
Mix ratio 100R:80H by weight; 100R:100H by volume ratio Resin to hardener
Mixed viscosity 45,000 cP ASTM D-2393; 25°C
Pot life 2 hours ASTM D-2471; 4 fl oz mass; 25°C
Technical properties

After-processing / final-state properties

Typical cured-material data. Cure and specimen preparation affect final properties; use the stated methods and conditions for interpretation.

Property Value Unit Method / condition
Ultimate tensile strength 33 MPa ASTM D-638; tested at 25°C
Elongation 9 % ASTM D-638; tested at 25°C
Glass-transition temperature (Tg) 63 °C DMA; ASTM D-4065
Hardness 80 Shore D ASTM D-2240
Coefficient of thermal expansion 8.5 × 10-5 1/°C ASTM E-831
Roller peel 4.9 N/mm ISO 4578; tested at 25°C