ARADUR HY 177

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARADUR HY 177

Main features

  • 600-900 mPa.s Component Viscosity
  • 40-60 Minute System Pot Life
  • Manual or Automatic System Metering

Product Description

ARADUR HY 177 Hardener is a modified polyamide liquid hardener used with ARALDITE GY 9708-1 in a room-temperature-curing epoxy casting system. The component is an amber-to-brown liquid with guideline viscosity of 600-900 mPa.s at 25 deg C, specific weight of 0.95-1.0 g/cm3 at 25 deg C, and a closed-cup flash point above 140 deg C. In the documented system, the mix ratio is 45 parts by weight or 52 parts by volume per 100 parts resin. The casting mixture offers a 40-60 minute pot life for 100 ml at 25 deg C. It is intended for casting or impregnation of transformers, filters, capacitors, and related electronic components.

Key features

  • Controlled component viscosity: Guideline viscosity is 600-900 mPa.s at 25 deg C by Brookfield measurement.
  • Practical system working time: The GY 9708-1/HY 177 mixture has a 40-60 minute pot life at 25 deg C.
  • Flexible processing setup: The documented system supports manual or automatic mixing and dosing.

Applications

As the hardener component in the ARALDITE GY 9708-1 system for casting or impregnation of transformers, filters, capacitors, and related electronic components.

Product Family

ARADUR HY 177

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark Amber Liquid
Color
Gardner
Physical Properties
Viscosity
600-890 mPa.s
Thermal Properties
Flash Point
160 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Guideline component values for ARADUR HY 177; cured-system data are excluded.

PropertyValueUnitMethod / condition
AppearanceAmber to brown liquidAs-supplied form
Viscosity600-900mPa.s25 deg C; ISO 2555:1989; Brookfield
Specific weight0.95-1.0g/cm325 deg C; ISO 2811-2:1997
Flash point> 140deg CClosed cup; DIN 51758