ARADUR HY 1300

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARADUR HY 1300

Main features

  • Specified 150-190 mPa.s Viscosity
  • 12.5-pbw System Mix Ratio
  • Casting and Vacuum-Casting Processing

Product Description

ARADUR HY 1300 Hardener is a formulated, medium-viscosity polyamine liquid hardener for use as the curing component in the documented ARALDITE CW 1304 casting system. At 25 deg C, the component has a specified viscosity of 150-190 mPa.s; specific gravity is 0.990-1.005 at 20 deg C, and appearance is a clear, yellowish liquid. In the CW 1304 system, it is mixed at 12.5 parts by weight per 100 parts resin for casting or vacuum-casting processes. The documented system is intended for inductive components, transformers, generators, motors, and encapsulation around metal or ceramic inserts. Values for cured castings remain specific to the stated resin pairing, mix ratio, and cure schedule.

Key features

  • Specified component viscosity: Viscosity is 150-190 mPa.s at 25 deg C under ISO 12058.
  • Low hardener loading: The CW 1304 system uses 12.5 parts hardener per 100 parts resin by weight.
  • Casting-process compatibility: The documented system supports casting and vacuum-casting electrical encapsulation.

Applications

As the hardener component in the ARALDITE CW 1304 system for inductive components, transformers, generators, motors, and metal- or ceramic-insert encapsulation.

Product Family

ARADUR HY 1300

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
150-190 mPa.s
General Properties
Appearance
clear, yellowish liquid
Mix Ratio
100 :23 by volume
Pot Life
21 minutes
Specific Gravity
0.990-1.005

Additional Information

Technical properties

As-supplied / before-processing properties

Specified component ranges for ARADUR HY 1300; cured-system data are excluded.

PropertyValueUnitMethod / condition
AppearanceClear, yellowish liquidVisual; specified range
Viscosity150-190mPa.s25 deg C; ISO 12058; specified range
Specific gravity0.990-1.00520 deg C; ISO 2811; specified range