ALPHA WS826

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA WS826

Main features

  • Eight-Hour High-Humidity Stencil Life
  • Air or Nitrogen Reflow
  • Zero-Halogen Water-Soluble Flux

Product Description

ALPHA WS-826 Solder Paste is a water-soluble, lead-free, zero-halogen solder paste developed for SAC305 assembly in air or nitrogen reflow. Type 4 and Type 5 powder options support fine-pitch printing, while the formulation maintains an eight-hour stencil life at both 25 deg C/50% RH and 30 deg C/70% RH. Its flux is classified ORM0 to IPC J-STD-004B, with no halides or halogens detected by the cited methods. Cold- and hot-slump testing passed without bridging above 0.20 mm and 0.25 mm, respectively. Residues are designed for hot deionized-water removal in batch or inline equipment after one or two reflow cycles. Properly stored unopened paste has a six-month shelf life at 0-10 deg C.

Key features

  • High-humidity stencil stability: Maintains eight-hour transfer efficiency at 30 deg C and 70% RH.
  • Air or nitrogen reflow: Supports SAC305 processing in either documented atmosphere.
  • Aqueous two-reflow cleanability: Residues are designed for hot deionized-water removal after one or two reflows.

Applications

SAC305 Type 4 or Type 5 SMT printing and air or nitrogen reflow with batch or inline aqueous cleaning.

Product Family

ALPHA WS826

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
SAC305

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AlloySAC305Available configuration
Powder sizesType 4; Type 5Available configurations
Flux classificationORM0IPC J-STD-004B
Halide / halogen contentNone detectedIPC J-STD-004B / BS EN 14582
Tack lifeConsistent over 24hoursJIS Z 3284
Ambient stencil life8hours25 deg C, 50% RH
Elevated-condition stencil life8hours30 deg C, 70% RH
Shelf life6monthsUnopened, refrigerated at 0-10 deg C