ALPHA WS362

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA WS362

Main features

  • High-activity, 25% solids water-soluble flux designed for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Highly water-soluble post-solder residues support effective cleaning for high ionic cleanliness and surface insulation resistance.
  • Halide-free formulation with rapid wetting and support for foam, spray, or wave application techniques.

Product Description

ALPHA WS362-25 Water-Soluble Surface Mount Flux is a halide-free, water-soluble organic flux designed for soldering surface mount and mixed technology assemblies where effective residue removal and high ionic cleanliness are important. Its high-activity, 25% solids formulation is recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures. After soldering, the highly water-soluble residues can be readily removed, supporting high ionic cleanliness and surface insulation resistance. ALPHA WS362-25 can be applied by foam, spray, or wave techniques and is designated ORMO according to IPC J-STD-004.

Key features

  • Highly water-soluble residue: Designed for effective post-solder cleaning where high ionic cleanliness is required.
  • High activity and 25% solids: Recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Halide-free formulation: Provides rapid wetting and carries an ORMO designation according to IPC J-STD-004.
  • Multiple application methods: Suitable for foam, spray, and wave application techniques.

Applications / Suitable for

  • Surface mount assemblies
  • Mixed technology assemblies
  • Densely packed assemblies requiring effective residue cleaning
  • Multilayer boards requiring relatively high preheat temperatures
Product Family

ALPHA WS362

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
25 %
Specific Gravity
0.846 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical properties of ALPHA WS362-25 in its as-supplied liquid state.

Property Value Unit Method or condition
Appearance Clear, pale yellow - As supplied
Solids content 25 wt/wt % Typical value
Specific gravity 0.846 +/- 0.005 - 25 °C (77 °F)
Acid number 33.00 +/- 2.00 mg KOH/g Typical value
pH 3.2 - 5% aqueous solution
Flash point 17 °C T.C.C.
Technical properties

After-processing / final-state properties

Surface insulation resistance results for ALPHA WS362-25 after hydrocleaning under the stated IPC J-STD-004 test conditions.

Property Result Requirement Method or condition
Surface insulation resistance - Comb-Down, hydrocleaned 4.4 x 108 ohms >1.0 x 108 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board
Surface insulation resistance - Control Boards 3.6 x 109 ohms >1.0 x 109 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board

Leading Brands Trust in Our Products and Services