ALPHA SM42-120P

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA SM42-120P

Main features

  • One-component, fast-curing epoxy surface mount adhesive designed for both screen printing and dispensing.
  • Non-sagging formulation with documented excellent adhesion, thermal resistance, and workability.
  • Cured material provides a Tg of 110 +/- 10 °C and insulation resistance greater than 1 x 10^12 ohms after 96 hours at 85 °C/85% RH.

Product Description

ALPHA HiTech SM42-120P Surface Mount Adhesive is a one-component, fast-curing epoxy adhesive designed for screen printing and dispensing in surface mount assembly. The red paste combines non-sagging behavior with documented adhesion, thermal resistance, and workability characteristics. It can be screen printed at room temperature or applied by dispensing, with full property development using the documented thermal cure schedules. ALPHA HiTech SM42-120P is also identified as halogen-free and compliant with RoHS Directive EU/2015/863.

Key features

  • Fast-curing one-component epoxy: Supplied as a ready-to-use red paste for surface mount adhesive applications.
  • Screen print and dispense capable: Can be effectively screen printed at room temperature and is also suitable for dispensing.
  • Non-sagging with strong functional properties: Documented features include non-sagging behavior, excellent adhesion, thermal resistance, and workability.
  • Halogen-free formulation: Identified as halogen-free and compliant with RoHS Directive EU/2015/863.

Applications / Suitable for

  • Surface mount adhesive applications
  • Screen printing at room temperature
  • Dispensing processes
Product Family

ALPHA SM42-120P

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Thixotropic index
≥ 3.0
Viscosity
55000–70000 Poise mPa.s
General Properties
Specific Gravity
1.2–1.4
Thermal Properties
Glass Transition Temperature (Tg)
110 ± 10 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical uncured material properties of ALPHA HiTech SM42-120P.

Property Value Unit Method / condition
Chemistry Epoxy - One-component surface mount adhesive
Appearance Red paste - Uncured
Viscosity 550 to 700 Poise Malcom PC-10A, 30 rpm at 25 °C
Specific gravity 1.2 to 1.4 - Typical uncured material property
Thixotropic index ≥ 3.0 - Typical uncured material property
Pot life 7 days 25 °C
Technical properties

After-processing / final-state properties

Selected typical cured material properties of ALPHA HiTech SM42-120P.

Property Value Unit Method / condition
Glass transition temperature (Tg) 110 +/- 10 °C DSC
CTE (α1), below Tg 65 +/- 10 ppm TMA
CTE (α2), above Tg 190 +/- 20 ppm TMA
Corrosion None - 96 hours at 40 °C, 95% RH
Moisture absorption < 1.0 wt% 24 hours, H2O at 25 °C
Insulation resistance >1 x 1012 ohms 96 hours at 85 °C, 85% RH
Hardness 80 to 90 Shore D Typical cured material property