ALPHA Vaculoy SAC305 Solder Bar

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

ALPHA Vaculoy SAC305 Solder Bar

Main features

  • Fast wetting
  • Excellent solderability
  • Very good drainage

Product Description

ALPHA SAC305 Solder Bar is a high-performance, lead-free alloy designed as a direct replacement for the industry-standard Sn63Pb37. It is the flagship of the SAC series (Tin-Silver-Copper), widely recognized for its excellent wetting characteristics and joint reliability in wave soldering and surface mount applications.

Product Key Features

  • Produced using the proprietary Vaculoy alloying process, which removes impurities—specifically oxides—to ensure low drossing and high-quality solder joints.
  • Fully lead-free and suitable for modern electronics manufacturing where environmental standards are a priority.
  • Fast wetting, in back to back tests 0.65s compared to 1.00s, for Sn/Cu-based materials
  • Excellent solderability due to fast wetting speed

Applications

  • Wave and selective soldering applications
Product Family

ALPHA SAC305 BAR

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
Shipping in 4 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Specific Heat Capacity
0.232 J/(g⋅°C)
General Properties
Density (g)
7.37 g/cm3