ALPHA NR330

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA NR330

Main features

  • VOC-Free Water-Based Processing
  • Low Bridging and Solder Balls
  • Non-Tacky Pin-Testable Residue

Product Description

ALPHA NR330 Liquid Soldering Flux is a VOC-free, water-based, halide-free, rosin- and resin-free low-solids no-clean flux for spray-applied wave soldering. Its activator system supports wetting and top-side hole fill on OSP-coated bare-copper boards, including boards exposed to prior reflow. Thermally stable activators help limit solder bridging, while surface-tension-reducing additives lower solder-ball formation. The formulation leaves a very low level of non-tacky residue for pin testing and board appearance. Typical as-supplied data include 4.0% solids, 1.013 +/- 0.003 specific gravity at 25 deg C, a 38.0 +/- 2.0 mg KOH/g acid number, and ORL0 classification.

Key features

  • OSP-board wetting: Supports wetting and top-side hole fill after prior thermal excursions.
  • Bridge and solder-ball control: Thermally stable activation and reduced surface tension address common wave-soldering defects.
  • Low non-tacky residue: Very low residue limits interference with pin testing.

Applications

Spray-applied wave soldering for lead-free and tin-lead electronic assemblies, including OSP-coated bare-copper boards.

Product Family

ALPHA NR330

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
4.0 %
Specific Gravity
1.013 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, colorless liquidTypical
Solids content4.0% by weightTypical
Specific gravity1.013 +/- 0.00325 deg C
Acid number38.0 +/- 2.0mg KOH/gTypical
pH2.35Typical
Flash pointNoneT.C.C.
Shelf life540daysFrom date of manufacture
Flux classificationORL0IPC J-STD-004