  • ALPHA K75-I provides a high-purity isopropyl alcohol and de-ionized water extract solution designed for ionic cleanliness testing in compliance with MIL-P-28809.
  • ALPHA K99-I provides a dedicated isopropyl-alcohol-based make-up solution for restoring K75-I to the desired alcohol/water ratio.
  • The complementary K75-I/K99-I system supports regular alcohol-percentage adjustment to maintain the accuracy of the ionic test instrument procedure.

Product Description

ALPHA K75-I and K99-I Test Solutions are complementary solutions used for ionic cleanliness testing and control of the test-solution alcohol/water ratio. ALPHA K75-I Extract Test Solution consists of high-purity isopropyl alcohol and de-ionized water and is designed for cleanliness testing in compliance with MIL-P-28809. ALPHA K99-I Ratio Adjusting Solution is an isopropyl-alcohol-based make-up solution used with the Solution Control Nomogram to restore K75-I to the desired alcohol/water ratio as alcohol is lost through evaporation. Regular monitoring and adjustment with K99-I helps maintain the accuracy of the ionic test instrument procedure.

Key features

  • Designed for ionic cleanliness testing: K75-I is formulated from high-purity isopropyl alcohol and de-ionized water for cleanliness testing in compliance with MIL-P-28809.
  • Controlled test-solution ratio: K99-I is designed to restore K75-I to the desired alcohol/water ratio as alcohol is lost through evaporation.
  • Supports test-procedure accuracy: Regular monitoring of alcohol percentage and adjustment with K99-I is used to maintain the ionic test instrument procedure.

Applications / Suitable for

  • Ionic cleanliness testing using ALPHA K75-I Extract Test Solution
  • Cleanliness testing in compliance with MIL-P-28809
  • Adjustment of K75-I alcohol/water ratio using ALPHA K99-I
Product Family

ALPHA K75I

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.2 %
Specific Gravity
0.790 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical physical properties of ALPHA K75-I and ALPHA K99-I test solutions.

Property Value Unit Product / condition
Solution type High-purity isopropyl alcohol and de-ionized water - ALPHA K75-I Extract Test Solution
Specific gravity 0.855 - ALPHA K75-I, 77 °F
Density 7.12 lb/gal ALPHA K75-I, 77 °F
Flash point 70 °F ALPHA K75-I
Volatile 100 % ALPHA K75-I
Solution type Isopropyl-alcohol-based make-up solution - ALPHA K99-I Ratio Adjusting Solution
Specific gravity 0.783 - ALPHA K99-I, 77 °F
Density 6.52 lb/gal ALPHA K99-I, 77 °F
Flash point 53 °F ALPHA K99-I
Volatile 100 % ALPHA K99-I