ALPHA EF8300LR

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA EF8300LR

Main features

  • Greater Than 96% Hole Fill
  • Low-Bridging Cu-OSP Soldering
  • Halide-Free Tack-Free Residue

Product Description

ALPHA EF-8300LR Liquid Soldering Flux is an active, halide-free, rosin- and resin-free, low-solids no-clean flux for wave soldering general and high-density circuit-board assemblies. It is designed for lead-free and eutectic tin-lead processes, including Cu-OSP boards. On 10 mil holes, demonstrated hole-fill yield exceeds 96%. The formulation also provides low bridging on connectors and bottom-side QFPs with good control of micro-solder balls. Spray or foam application leaves an evenly spread, tack-free, pin-testable residue. At 25 deg C, typical specific gravity is 0.801 +/- 0.003; the solids level is 4.0%, with ORM0 classification.

Key Features

  • Cu-OSP process support: Specifically designed for wave soldering Cu-OSP circuit boards.
  • High-density soldering: Greater than 96% hole-fill yield on 10 mil holes with low connector bridging.
  • Halide-free low residue: Rosin- and resin-free formulation leaves tack-free, pin-testable residue.

Applications

Spray- or foam-applied wave soldering for general and high-density lead-free or tin-lead assemblies, including Cu-OSP circuit boards.

Product Family

ALPHA EF8300LR

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
4.0 %
Specific Gravity
0.801 ± 0.003 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, pale yellow liquidVisual
Solids content4.0% by weightTypical
Specific gravity0.801 +/- 0.00325 deg C
Acid number32.0 +/- 2.0mg KOH/gTypical
pH3.05% v/v aqueous solution
Flash point17deg CT.C.C.
Shelf life360daysTypical
Flux classificationORM0IPC J-STD-004