ALPHA EF6100

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF6100

Main features

  • Alloy-Specific Wave Process Control
  • Low-Solids Pin-Testable Residue
  • High-Reliability No-Clean Soldering

Product Description

ALPHA EF-6100 Liquid Soldering Flux is a low-solids, no-clean, alcohol-based flux for lead-free and tin-lead wave and selective soldering. It is applied by spray and is designed for through-hole fill with reduced solder balling, bridging, and skips while leaving low residues compatible with pin testing. Typical solids content is 3.8%, and the acid number is controlled to 22.8 to 25.2 to maintain solids during use. Process guidance separates SAC305/SACX0307 and Sn63Pb37 settings, including alloy-specific flux loading, preheat, contact time, and solder-pot temperature. Residues are designed to remain on the board but can be removed with aqueous or solvent cleaners when needed.

Key features

  • Alloy-specific spray process: Separate SAC305/SACX0307 and Sn63Pb37 settings define flux loading, preheat, contact time, and solder-pot conditions.
  • Low-solids no-clean residue: A 3.8% solids formulation leaves low residue for no-clean assembly and supports pin-test access.
  • SIR and electromigration performance: Uncleaned residues pass the listed IPC, Bellcore, and JIS surface-insulation-resistance and electromigration tests under specified conditions.

Applications

Used for lead-free and tin-lead wave or selective soldering where spray fluxing, controlled alloy-specific process settings, and low no-clean residue are required.

Product Family

ALPHA EF6100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
3.8 %
Specific Gravity
0.794 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, colorless to pale yellow liquidTypical
Solids content3.8% by weightTypical
Specific gravity0.794 +/- 0.003At 25 deg C (77 deg F)
Acid number23.9 +/- 1.2mg KOH/gTypical
pH3.35% aqueous solution
Flash point12 (53)deg C (deg F)T.C.C.
Shelf life360daysFrom date of manufacture
IPC classificationORL0IPC J-STD-004