ALPHA EF-9301

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA EF-9301

Main features

  • Greater Than 95% Hole Fill
  • Low-Bridging SMT Soldering
  • Spray or Foam Fluxing

Product Description

ALPHA EF-9301 Liquid Soldering Flux is a rosin-containing, ready-to-use liquid flux developed for full-dulling wave soldering with tin-lead and lead-free alloys. Spray or foam application produces smooth, dull solder joints with evenly spread, low-tack residue. On connectors and bottom-side SMT components, the flux shows low bridging together with strong hole fill and low solder balling. Hole-fill yield is greater than 95% on 10 mil holes. The typical solids level is 7.0%, with specific gravity of 0.798 +/- 0.005 at 25 deg C and ROM1 classification. Separate process recommendations cover preheat and solder-pot temperatures for tin-lead and lead-free operation.

Key Features

  • High hole-fill yield: Greater than 95% hole-fill yield on 10 mil holes.
  • Low-bridging soldering: Low bridging on connectors and bottom-side SMT components.
  • Flexible flux application: Ready for spray or foam application in tin-lead and lead-free processes.

Applications

Wave soldering with tin-lead and lead-free alloys using spray or foam flux application.

Product Family

ALPHA EF-9301

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
7.0 %
Specific Gravity
0.798 ± 0.005 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, pale yellow liquidVisual
Solids content7.0% by weightTypical
Specific gravity0.798 +/- 0.00525 deg C
Acid number16 to 17mg KOH/gTypical
pH3.6Typical
Flash point12deg CT.C.C.
Shelf life360daysTypical
Flux classificationROM1J-STD-004

Leading Brands Trust in Our Products and Services