ALPHA EF-8800HF No Clean Flux
Harmonization Code : 3810.90.90 | Fluxes and other auxiliary preparations for soldering, brazing, welding
Main features
- Robust soldering performance
- Evenly spread, tack free residue
- Halide-free
Product Description
ALPHA EF-8800HF is an alcohol based flux for both standard and thicker, high density Pb-free PCB processes. EF-8800HF exhibits stable performance even under long exposure to higher preheat and higher solder pot temperature. ALPHA EF-8800HF is formulated to have low bridging on bottom side QFPs, as well as provide superior performance in pin testing, hole-fill and solderballing. Additionally, it provides good Pb-free solder joint cosmetics with an evenly spread, tack free residue.
Product Key Features
- Robust soldering performance even under high top-side preheat >125 oC
- Low bridging performance on connectors, 0.65 mm and 0.80 mm QFPs
- Pin testable
- Halide-free
Applications
- Wave solder flux for thick board applications
Packaging
Please select Package Type.
Technical Specifications
General Properties
Appearance
Clear, pale yellow liquid
Solids
6.0 %
Specific Gravity
0.799
Thermal Properties
Flash Point
17 °C